General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 1.8 % Show Supplier Material materials with Absorción de agua of 1.8 % | dry | ISO 62 | at 23°C after 24h |
6.7 % Show Supplier Material materials with Absorción de agua of 6.7 % | dry | Sim. to ISO 62 | ||
Densidad | 1.49 g/cm³ Show Supplier Material materials with Densidad of 1.49 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2.3 % Show Supplier Material materials with Moisture absorption of 2.3 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|---|
Elongación | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | dry | 1 mm | ISO 527-1/-2 | ||
2.6 % Show Supplier Material materials with Elongación of 2.6 % | dry | 1 mm | ISO 527-1/-2 | |||
3.6 % Show Supplier Material materials with Elongación of 3.6 % | conditioned | ISO 527-1/-2 | ||||
Módulo de flexión | 8 GPa Show Supplier Material materials with Módulo de flexión of 8 GPa | conditioned | ISO 178 | |||
12.5 GPa Show Supplier Material materials with Módulo de flexión of 12.5 GPa | dry | ISO 178 | ||||
Módulo elástico | 8 GPa Show Supplier Material materials with Módulo elástico of 8 GPa | conditioned | ISO 527-1/-2 | |||
12.5 GPa Show Supplier Material materials with Módulo elástico of 12.5 GPa | dry | 1 mm | ISO 527-1/-2 | |||
12.5 GPa Show Supplier Material materials with Módulo elástico of 12.5 GPa | dry | 1 mm | ISO 527-1/-2 | |||
Resistencia a la tracción | 140 MPa Show Supplier Material materials with Resistencia a la tracción of 140 MPa | conditioned | ISO 527-1/-2 | |||
200 MPa Show Supplier Material materials with Resistencia a la tracción of 200 MPa | dry | 1 mm | ISO 527-1/-2 | |||
210 MPa Show Supplier Material materials with Resistencia a la tracción of 210 MPa | dry | 1 mm | ISO 527-1/-2 | at low thickness | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13 kJ/m² | conditioned | ISO 179/1eA | |||
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m² | dry | ISO 179/1eU | ||
23 °C | 70 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 70 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 3.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
4e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.75 mm | ||
Temperatura de flexión bajo carga | 290 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 290 °C | dry | ISO 75-1/-2 | 2 MPa | ||
290 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 290 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4.4 [-] Show Supplier Material materials with Constante dieléctrica of 4.4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.8 [-] Show Supplier Material materials with Constante dieléctrica of 4.8 [-] | dry | IEC 62631-2-1 | 100Hz | |
5.2 [-] Show Supplier Material materials with Constante dieléctrica of 5.2 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
11.2 [-] Show Supplier Material materials with Constante dieléctrica of 11.2 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 80 [-] Show Supplier Material materials with Factor de disipación of 80 [-] | dry | IEC 62631-2-1 | 100Hz |
170 [-] Show Supplier Material materials with Factor de disipación of 170 [-] | dry | IEC 62631-2-1 | 1MHz | |
850 [-] Show Supplier Material materials with Factor de disipación of 850 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
1400 [-] Show Supplier Material materials with Factor de disipación of 1400 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Rigidez dieléctrica | 30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | conditioned | IEC 60243-1 | |
33 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 33 kV/mm | dry | IEC 60243-1 | ||
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | ||
Índice de seguimiento comparativo | 425 V Show Supplier Material materials with Índice de seguimiento comparativo of 425 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Reflow connectors (2) | |
Certifications | Yellow Card Available | |
Fillers | 35% Glass Fiber |