General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 3.9 % Show Supplier Material materials with Absorción de agua of 3.9 % | dry | Sim. to ISO 62 |
Densidad | 1.45 g/cm³ Show Supplier Material materials with Densidad of 1.45 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.4 % Show Supplier Material materials with Moisture absorption of 1.4 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 2.4 % Show Supplier Material materials with Elongación of 2.4 % | dry | ISO 527-1/-2 |
2.3 % Show Supplier Material materials with Elongación of 2.3 % | dry | ISO 527-1/-2 | ||
2.4 % Show Supplier Material materials with Elongación of 2.4 % | conditioned | ISO 527-1/-2 | ||
80 °C | 2.8 % Show Supplier Material materials with Elongación of 2.8 % | dry | ISO 527-1/-2 | |
100 °C | 3.8 % Show Supplier Material materials with Elongación of 3.8 % | dry | ISO 527-1/-2 | |
120 °C | 4.5 % Show Supplier Material materials with Elongación of 4.5 % | dry | ISO 527-1/-2 | |
140 °C | 4.5 % Show Supplier Material materials with Elongación of 4.5 % | dry | ISO 527-1/-2 | |
160 °C | 4.5 % Show Supplier Material materials with Elongación of 4.5 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 230 MPa Show Supplier Material materials with Flexural yield strength of 230 MPa | dry | ISO 178 | |
Módulo de flexión | 10 GPa Show Supplier Material materials with Módulo de flexión of 10 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 12 GPa Show Supplier Material materials with Módulo elástico of 12 GPa | dry | ISO 527-1/-2 |
11 GPa Show Supplier Material materials with Módulo elástico of 11 GPa | conditioned | ISO 527-1/-2 | ||
11.5 GPa Show Supplier Material materials with Módulo elástico of 11.5 GPa | dry | ISO 527-1/-2 | ||
80 °C | 9 GPa Show Supplier Material materials with Módulo elástico of 9 GPa | dry | ISO 527-1/-2 | |
100 °C | 7 GPa Show Supplier Material materials with Módulo elástico of 7 GPa | dry | ISO 527-1/-2 | |
120 °C | 5.5 GPa Show Supplier Material materials with Módulo elástico of 5.5 GPa | dry | ISO 527-1/-2 | |
140 °C | 4.7 GPa Show Supplier Material materials with Módulo elástico of 4.7 GPa | dry | ISO 527-1/-2 | |
160 °C | 4.2 GPa Show Supplier Material materials with Módulo elástico of 4.2 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 180 MPa Show Supplier Material materials with Resistencia a la tracción of 180 MPa | dry | ISO 527-1/-2 |
145 MPa Show Supplier Material materials with Resistencia a la tracción of 145 MPa | conditioned | ISO 527-1/-2 | ||
155 MPa Show Supplier Material materials with Resistencia a la tracción of 155 MPa | dry | ISO 527-1/-2 | ||
80 °C | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | dry | ISO 527-1/-2 | |
100 °C | 85 MPa Show Supplier Material materials with Resistencia a la tracción of 85 MPa | dry | ISO 527-1/-2 | |
120 °C | 70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | dry | ISO 527-1/-2 | |
140 °C | 60 MPa Show Supplier Material materials with Resistencia a la tracción of 60 MPa | dry | ISO 527-1/-2 | |
160 °C | 55.0 MPa Show Supplier Material materials with Resistencia a la tracción of 55.0 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | dry, conditioned | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 55.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 55.0 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
7e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Conductividad térmica | 0.35 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.35 W/(m·K) | dry | ASTM E1461 | through plane | ||
0.41 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.41 W/(m·K) | dry | ASTM E1461 | in plane | |||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 3 mm | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.4 mm | |||
Inflamabilidad | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 150 °C Show Supplier Material materials with Relative temperature index, electrical of 150 °C | dry | UL746B | 0.75 mm | ||
Temperatura de flexión bajo carga | 275 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 275 °C | dry | ISO 75-1/-2 | 2 MPa | ||
300 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 300 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 325 °C Show Supplier Material materials with Temperatura de fusión of 325 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.6 [-] Show Supplier Material materials with Constante dieléctrica of 3.6 [-] | dry | IEC 60250 | 10GHz |
3.7 [-] Show Supplier Material materials with Constante dieléctrica of 3.7 [-] | dry | IEC 60250 | 1GHz | |
3.75 [-] Show Supplier Material materials with Constante dieléctrica of 3.75 [-] | conditioned | IEC 60250 | 10GHz | |
3.9 [-] Show Supplier Material materials with Constante dieléctrica of 3.9 [-] | conditioned | IEC 60250 | 1GHz | |
Factor de disipación | 100 [-] Show Supplier Material materials with Factor de disipación of 100 [-] | dry | IEC 60250 | 10GHz |
140 [-] Show Supplier Material materials with Factor de disipación of 140 [-] | dry | IEC 60250 | 1GHz | |
150 [-] Show Supplier Material materials with Factor de disipación of 150 [-] | conditioned | IEC 60250 | 10GHz | |
200 [-] Show Supplier Material materials with Factor de disipación of 200 [-] | conditioned | IEC 60250 | 1GHz | |
Rigidez dieléctrica | 33 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 33 kV/mm | dry | IEC 60243-1 | |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry, conditioned | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Reflow connectors, DDR DIMM Connectors, Audio Jack Connectors, Reflow connectors (2), Reflow connectors (3) | |
Certifications | Yellow Card Available | |
Fillers | 30% Glass Fiber |