General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 66 % Show Supplier Material materials with Bio-based content of 66 % | dry | ASTM D6866-12 Method B |
Densidad | 1.08 g/cm³ Show Supplier Material materials with Densidad of 1.08 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.8 % Show Supplier Material materials with Moisture absorption of 1.8 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 78 [-] Show Supplier Material materials with Dureza Shore D of 78 [-] | dry | ISO 868 | 15s | |
Elongación | 45 % Show Supplier Material materials with Elongación of 45 % | dry | ISO 527-1/-2 | ||
50 % Show Supplier Material materials with Elongación of 50 % | conditioned | ISO 527-1/-2 | |||
Flexural yield strength | 50 MPa Show Supplier Material materials with Flexural yield strength of 50 MPa | conditioned | ISO 178 | ||
95 MPa Show Supplier Material materials with Flexural yield strength of 95 MPa | dry | ISO 178 | |||
Módulo de flexión | 1.3 GPa Show Supplier Material materials with Módulo de flexión of 1.3 GPa | conditioned | ISO 178 | ||
2.4 GPa Show Supplier Material materials with Módulo de flexión of 2.4 GPa | dry | ISO 178 | |||
Módulo elástico | 1.3 GPa Show Supplier Material materials with Módulo elástico of 1.3 GPa | conditioned | ISO 527-1/-2 | ||
2.5 GPa Show Supplier Material materials with Módulo elástico of 2.5 GPa | dry | ISO 527-1/-2 | |||
Resistencia a la tracción | 50 MPa Show Supplier Material materials with Resistencia a la tracción of 50 MPa | conditioned | ISO 527-1/-2 | ||
65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | dry | ISO 527-1/-2 | |||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | dry | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 20 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 20 kJ/m² | conditioned | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 76 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 76 °C | dry | ISO 75-1/-2 | 2 MPa | |
165 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 165 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 250 °C Show Supplier Material materials with Temperatura de fusión of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | conditioned | IEC 60243-1 |
34 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 34 kV/mm | dry | IEC 60243-1 | |
Volume resistivity | 1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | conditioned | IEC 62631-3-1 |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | conditioned | IEC 60112 |
Rheological Properties
Technological properties
Property |
---|