General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 2.25 % Show Supplier Material materials with Absorción de agua of 2.25 % | dry | ISO 62 | at 23°C after 24h |
8.1 % Show Supplier Material materials with Absorción de agua of 8.1 % | dry | Sim. to ISO 62 | ||
Densidad | 1.36 g/cm³ Show Supplier Material materials with Densidad of 1.36 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2.2 % Show Supplier Material materials with Moisture absorption of 2.2 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 1.5 % Show Supplier Material materials with Elongación of 1.5 % | dry | ISO 527-1/-2 |
1.6 % Show Supplier Material materials with Elongación of 1.6 % | dry | ISO 527-1/-2 | ||
3.5 % Show Supplier Material materials with Elongación of 3.5 % | conditioned | ISO 527-1/-2 | ||
120 °C | 3.1 % Show Supplier Material materials with Elongación of 3.1 % | dry | ISO 527-1/-2 | |
160 °C | 3.1 % Show Supplier Material materials with Elongación of 3.1 % | dry | ISO 527-1/-2 | |
180 °C | 3.1 % Show Supplier Material materials with Elongación of 3.1 % | dry | ISO 527-1/-2 | |
200 °C | 3.1 % Show Supplier Material materials with Elongación of 3.1 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 240 MPa Show Supplier Material materials with Flexural yield strength of 240 MPa | conditioned | ISO 178 | |
340 MPa Show Supplier Material materials with Flexural yield strength of 340 MPa | dry | ISO 178 | ||
120 °C | 200 MPa Show Supplier Material materials with Flexural yield strength of 200 MPa | dry | ISO 178 | |
160 °C | 170 MPa Show Supplier Material materials with Flexural yield strength of 170 MPa | dry | ISO 178 | |
Módulo de flexión | 12.5 GPa Show Supplier Material materials with Módulo de flexión of 12.5 GPa | conditioned | ISO 178 | |
21 GPa Show Supplier Material materials with Módulo de flexión of 21 GPa | dry | ISO 178 | ||
120 °C | 10.5 GPa Show Supplier Material materials with Módulo de flexión of 10.5 GPa | dry | ISO 178 | |
160 °C | 10 GPa Show Supplier Material materials with Módulo de flexión of 10 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 23.5 GPa Show Supplier Material materials with Módulo elástico of 23.5 GPa | dry | ISO 527-1/-2 |
14.5 GPa Show Supplier Material materials with Módulo elástico of 14.5 GPa | conditioned | ISO 527-1/-2 | ||
23.5 GPa Show Supplier Material materials with Módulo elástico of 23.5 GPa | dry | ISO 527-1/-2 | ||
120 °C | 12.5 GPa Show Supplier Material materials with Módulo elástico of 12.5 GPa | dry | ISO 527-1/-2 | |
160 °C | 11 GPa Show Supplier Material materials with Módulo elástico of 11 GPa | dry | ISO 527-1/-2 | |
180 °C | 10.5 GPa Show Supplier Material materials with Módulo elástico of 10.5 GPa | dry | ISO 527-1/-2 | |
200 °C | 10 GPa Show Supplier Material materials with Módulo elástico of 10 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 265 MPa Show Supplier Material materials with Resistencia a la tracción of 265 MPa | dry | ISO 527-1/-2 |
160 MPa Show Supplier Material materials with Resistencia a la tracción of 160 MPa | conditioned | ISO 527-1/-2 | ||
250 MPa Show Supplier Material materials with Resistencia a la tracción of 250 MPa | dry | ISO 527-1/-2 | ||
120 °C | 130 MPa Show Supplier Material materials with Resistencia a la tracción of 130 MPa | dry | ISO 527-1/-2 | |
160 °C | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | dry | ISO 527-1/-2 | |
180 °C | 100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | dry | ISO 527-1/-2 | |
200 °C | 90 MPa Show Supplier Material materials with Resistencia a la tracción of 90 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | dry | ISO 179/1eA | |
23 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 50 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 50 kJ/m² | dry | ISO 179/1eU |
-30 °C | 55.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 55.0 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 50 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 50 kJ/m² | dry | ISO 179/1eU | |
23 °C | 80 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 80 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
3.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Temperatura de flexión bajo carga | 290 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 290 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | dry | ISO 294-4 | Parallel |
0.6 % Show Supplier Material materials with Contracción of 0.6 % | dry | ISO 294-4 | Normal | |
Viscosity number | 150 cm³/gr Show Supplier Material materials with Viscosity number of 150 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 30% Carbon Fiber and PTFE |