General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 2.4 % Show Supplier Material materials with Absorción de agua of 2.4 % | dry | ISO 62 | at 23°C after 24h |
8.6 % Show Supplier Material materials with Absorción de agua of 8.6 % | dry | Sim. to ISO 62 | ||
Densidad | 1.43 g/cm³ Show Supplier Material materials with Densidad of 1.43 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2.35 % Show Supplier Material materials with Moisture absorption of 2.35 % | dry | Sim. to ISO 62 | |
Índice límite de óxigeno | 29.0 % Show Supplier Material materials with Índice límite de óxigeno of 29.0 % | dry | ISO 4589-1/-2 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 7 % Show Supplier Material materials with Elongación of 7 % | dry | ISO 527-1/-2 | |
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 130 MPa Show Supplier Material materials with Flexural yield strength of 130 MPa | dry | ISO 178 | |
Módulo de flexión | 3.2 GPa Show Supplier Material materials with Módulo de flexión of 3.2 GPa | dry | ISO 178 | |
Módulo elástico | 3.4 GPa Show Supplier Material materials with Módulo elástico of 3.4 GPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | dry | ISO 179/1eA |
23 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 8e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
9e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Inflamabilidad | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Temperatura de flexión bajo carga | 190 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 190 °C | dry | ISO 75-1/-2 | 2 MPa | ||
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.5 [-] Show Supplier Material materials with Constante dieléctrica of 3.5 [-] | dry | IEC 62631-2-1 | 1MHz |
3.8 [-] Show Supplier Material materials with Constante dieléctrica of 3.8 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.1 [-] Show Supplier Material materials with Constante dieléctrica of 4.1 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
10 [-] Show Supplier Material materials with Constante dieléctrica of 10 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 50 [-] Show Supplier Material materials with Factor de disipación of 50 [-] | dry | IEC 62631-2-1 | 100Hz |
200 [-] Show Supplier Material materials with Factor de disipación of 200 [-] | dry | IEC 62631-2-1 | 1MHz | |
800 [-] Show Supplier Material materials with Factor de disipación of 800 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
2800 [-] Show Supplier Material materials with Factor de disipación of 2800 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Rigidez dieléctrica | 25 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 25 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | dry | IEC 60243-1 | ||
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+07 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+07 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | ||
Índice de seguimiento comparativo | 225 V Show Supplier Material materials with Índice de seguimiento comparativo of 225 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 1.5 % Show Supplier Material materials with Contracción of 1.5 % | dry | Sim. to ISO 294-4 | Parallel |
1.5 % Show Supplier Material materials with Contracción of 1.5 % | dry | Sim. to ISO 294-4 | Normal | |
Density of melt | 1140 g/cm³ Show Supplier Material materials with Density of melt of 1140 g/cm³ | dry | - | |
Thermal conductivity of melt | 0.24 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.24 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |