General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.38 g/cm³ Show Supplier Material materials with Densidad of 1.38 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2.8 % Show Supplier Material materials with Elongación of 2.8 % | dry | ISO 527-1/-2 | |
Módulo elástico | 6.5 GPa Show Supplier Material materials with Módulo elástico of 6.5 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure |
---|---|---|---|---|
Temperatura de flexión bajo carga | 183 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 183 °C | dry | ISO 75-1/-2 | 2 MPa |
Technological properties
Property | ||
---|---|---|
Fillers | 20% Glass Fiber |