General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.26 g/cm³ Show Supplier Material materials with Densidad of 1.26 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 5 % Show Supplier Material materials with Elongación of 5 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 90 MPa Show Supplier Material materials with Flexural yield strength of 90 MPa | dry | ISO 178 | |
Módulo de flexión | 3 GPa Show Supplier Material materials with Módulo de flexión of 3 GPa | dry | ISO 178 | |
Módulo elástico | 3.2 GPa Show Supplier Material materials with Módulo elástico of 3.2 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 50 MPa Show Supplier Material materials with Resistencia a la tracción of 50 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 3.3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3.3 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|
Inflamabilidad | V-0 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes |
Temperatura de fusión | 325 °C Show Supplier Material materials with Temperatura de fusión of 325 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 125 °C Show Supplier Material materials with Temperatura de transición del vidrio of 125 °C | dry | ISO 11357-1/-2 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 1.5 % Show Supplier Material materials with Contracción of 1.5 % | dry | ISO 294-4 | Parallel |
2 % Show Supplier Material materials with Contracción of 2 % | dry | ISO 294-4 | Normal | |
Viscosity number | 98 cm³/gr Show Supplier Material materials with Viscosity number of 98 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |