General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.8 % Show Supplier Material materials with Absorción de agua of 0.8 % | dry | Sim. to ISO 62 |
Densidad | 0.65 g/cm³ Show Supplier Material materials with Densidad of 0.65 g/cm³ | dry | ISO 60 |
1.08 g/cm³ Show Supplier Material materials with Densidad of 1.08 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore A | 85 [-] Show Supplier Material materials with Dureza Shore A of 85 [-] | dry | ISO 868 | 3s |
Dureza Shore D | 25 [-] Show Supplier Material materials with Dureza Shore D of 25 [-] | dry | ISO 868 | 3s |
Elongación | 300 % Show Supplier Material materials with Elongación of 300 % | dry | ISO 527-1/-2 | |
900 % Show Supplier Material materials with Elongación of 900 % | dry | ISO 527-1/-2 | ||
Módulo elástico | 0.03 GPa Show Supplier Material materials with Módulo elástico of 0.03 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 16 MPa Show Supplier Material materials with Resistencia a la tracción of 16 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2.2e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
2.2e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Inflamabilidad | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes |
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | UL746B | 2 mm | |
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | UL746B | 2 mm | |
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | UL746B | 2 mm | |
Temperatura de fusión | 180 °C Show Supplier Material materials with Temperatura de fusión of 180 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | -80 °C Show Supplier Material materials with Temperatura de transición del vidrio of -80 °C | dry | ISO 11357-1/-2 | 10°C/min | |
-74 °C Show Supplier Material materials with Temperatura de transición del vidrio of -74 °C | dry | ASTM D5026/D7028 | DMTA (tan d) |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Volume resistivity | 5e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 5e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Density of melt | 905 g/cm³ Show Supplier Material materials with Density of melt of 905 g/cm³ | dry | - | |
Velocidad de flujo del volumen derretido | 230 °C | 45 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 45 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |