General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 4.1 % Show Supplier Material materials with Absorción de agua of 4.1 % | dry | Sim. to ISO 62 |
Densidad | 1.63 g/cm³ Show Supplier Material materials with Densidad of 1.63 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.9 % Show Supplier Material materials with Moisture absorption of 0.9 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 0.6 % Show Supplier Material materials with Elongación of 0.6 % | dry | ISO 527-1/-2 | |
Módulo elástico | 12.5 GPa Show Supplier Material materials with Módulo elástico of 12.5 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 55.0 MPa Show Supplier Material materials with Resistencia a la tracción of 55.0 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 2 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 2 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
2.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Conductividad térmica | 1 W/(m·K) Show Supplier Material materials with Conductividad térmica of 1 W/(m·K) | dry | ASTM E1461 | through plane | |
8 W/(m·K) Show Supplier Material materials with Conductividad térmica of 8 W/(m·K) | dry | ASTM E1461 | in plane | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.75 mm | |
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 3 mm | ||
Glow Wire Ignition Temperature | 825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | dry | IEC 60695-2-13 | 0.75 mm | |
900 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 900 °C | dry | IEC 60695-2-13 | 3 mm | ||
Inflamabilidad | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes |
5VA | dry | IEC 60695-11-20 | 1.6 mm | ||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | UL746B | 0.75 mm | |
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | dry | UL746B | 0.75 mm | |
Relative temperature index, mechanical strength | 120 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 120 °C | dry | UL746B | 0.75 mm |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | dry | IEC 60243-1 |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Heat Sinks in LED Lamps | |
Certifications | Yellow Card Available |