General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.25 g/cm³ Show Supplier Material materials with Densidad of 1.25 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 62 [-] Show Supplier Material materials with Dureza Shore D of 62 [-] | dry | ISO 868 | 3s | |
Elongación | 365 % Show Supplier Material materials with Elongación of 365 % | dry | ISO 527-1/-2 | ||
Elongation at yield | 24 % Show Supplier Material materials with Elongation at yield of 24 % | dry | ISO 527-1/-2 | ||
Módulo elástico | 0.43 GPa Show Supplier Material materials with Módulo elástico of 0.43 GPa | dry | ISO 527-1/-2 | ||
Resistencia a desgarros | 150 kN/m Show Supplier Material materials with Resistencia a desgarros of 150 kN/m | dry | ISO 34-1; Method B | ||
Resistencia a la tracción | 35 MPa Show Supplier Material materials with Resistencia a la tracción of 35 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | dry | ISO 179/1eA | |
23 °C | 23 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 23 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|
Inflamabilidad | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes |
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | 2 mm | UL746B | |
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | 2 mm | UL746B | |
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | 2 mm | UL746B | |
Temperatura de fusión | 221 °C Show Supplier Material materials with Temperatura de fusión of 221 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 230 °C | 26 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 26 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Bed Springs | |
Certifications | Yellow Card Available |