General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 9 % Show Supplier Material materials with Absorción de agua of 9 % | dry | Sim. to ISO 62 |
Densidad | 1.14 g/cm³ Show Supplier Material materials with Densidad of 1.14 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.5 % Show Supplier Material materials with Moisture absorption of 2.5 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 14.0 % Show Supplier Material materials with Elongación of 14.0 % | dry | ISO 527-1/-2 | |
Elongation at yield | 3 % Show Supplier Material materials with Elongation at yield of 3 % | dry | ISO 527-1/-2 | |
Módulo elástico | 3 GPa Show Supplier Material materials with Módulo elástico of 3 GPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Ball pressure temperature | 180 °C Show Supplier Material materials with Ball pressure temperature of 180 °C | dry | IEC 60695-10-2 | |||
Glow Wire Flammability Index | 675 °C Show Supplier Material materials with Glow Wire Flammability Index of 675 °C | dry | IEC 60695-2-12 | 3 mm | ||
725 °C Show Supplier Material materials with Glow Wire Flammability Index of 725 °C | dry | IEC 60695-2-12 | 0.75 mm | |||
Temperatura de flexión bajo carga | 60 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 60 °C | dry | ISO 75-1/-2 | 2 MPa | ||
150 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 150 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Índice de seguimiento comparativo | 575 V Show Supplier Material materials with Índice de seguimiento comparativo of 575 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.1 % Show Supplier Material materials with Contracción of 1.1 % | dry | ISO 294-4 | Parallel | |
1.1 % Show Supplier Material materials with Contracción of 1.1 % | dry | ISO 294-4 | Normal | ||
Velocidad de flujo del volumen derretido | 235 °C | 90 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 90 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Surfboard components |