General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.55 % Show Supplier Material materials with Absorción de agua of 0.55 % | dry | Sim. to ISO 62 |
Densidad | 1.29 g/cm³ Show Supplier Material materials with Densidad of 1.29 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.25 % Show Supplier Material materials with Moisture absorption of 0.25 % | dry | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 56.0 [-] Show Supplier Material materials with Dureza Shore D of 56.0 [-] | dry | ISO 868 | 15s |
Elongation at yield | 18 % Show Supplier Material materials with Elongation at yield of 18 % | dry | ISO 527-1/-2 | |
Módulo de flexión | 0.9 GPa Show Supplier Material materials with Módulo de flexión of 0.9 GPa | dry | ISO 178 | |
Módulo elástico | 1 GPa Show Supplier Material materials with Módulo elástico of 1 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 18 MPa Show Supplier Material materials with Resistencia a la tracción of 18 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 110 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 110 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 185 °C Show Supplier Material materials with Temperatura de fusión of 185 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo de la masa derretida | 230 °C | 24 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 24 g/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Chair Carriers, Seat Suspension/Fabrics | |
Fillers | Glass Fiber |