General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 33 % Show Supplier Material materials with Absorción de agua of 33 % | dry | Sim. to ISO 62 |
Densidad | 1.25 g/cm³ Show Supplier Material materials with Densidad of 1.25 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 45 [-] Show Supplier Material materials with Dureza Shore D of 45 [-] | dry | ISO 868 | 3s |
Elongación | 280 % Show Supplier Material materials with Elongación of 280 % | dry | ISO 527-1/-2 | |
Módulo elástico | 0.11 GPa Show Supplier Material materials with Módulo elástico of 0.11 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 20 MPa Show Supplier Material materials with Resistencia a la tracción of 20 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 185 °C Show Supplier Material materials with Temperatura de fusión of 185 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 44 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 44 °C | dry | ISO 306 | 50°C/h 50N |
156 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 156 °C | dry | ISO 306 | 50°C/h 10N |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 230 °C | 10 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 10 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Roofing membranes, Breathable Outdoor clothing, Breathable Films for Food Packaging, Smokable Sausage Casings | |
Certifications | Food Contact, USP class VI |