General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.47 g/cm³ Show Supplier Material materials with Densidad of 1.47 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 2.7 % Show Supplier Material materials with Elongación of 2.7 % | dry | ISO 527-1/-2 |
2.7 % Show Supplier Material materials with Elongación of 2.7 % | dry | ISO 527-1/-2 | ||
4 % Show Supplier Material materials with Elongación of 4 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 160 MPa Show Supplier Material materials with Flexural yield strength of 160 MPa | conditioned | ISO 178 | |
230 MPa Show Supplier Material materials with Flexural yield strength of 230 MPa | dry | ISO 178 | ||
Módulo de flexión | 7.8 GPa Show Supplier Material materials with Módulo de flexión of 7.8 GPa | conditioned | ISO 178 | |
11.2 GPa Show Supplier Material materials with Módulo de flexión of 11.2 GPa | dry | ISO 178 | ||
Módulo elástico | -40 °C | 12 GPa Show Supplier Material materials with Módulo elástico of 12 GPa | dry | ISO 527-1/-2 |
7.5 GPa Show Supplier Material materials with Módulo elástico of 7.5 GPa | conditioned | ISO 527-1/-2 | ||
11.5 GPa Show Supplier Material materials with Módulo elástico of 11.5 GPa | dry | ISO 527-1/-2 | ||
40 °C | 11 GPa Show Supplier Material materials with Módulo elástico of 11 GPa | dry | ISO 527-1/-2 | |
100 °C | 5.2 GPa Show Supplier Material materials with Módulo elástico of 5.2 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 190 MPa Show Supplier Material materials with Resistencia a la tracción of 190 MPa | dry | ISO 527-1/-2 |
90 MPa Show Supplier Material materials with Resistencia a la tracción of 90 MPa | conditioned | ISO 527-1/-2 | ||
140 MPa Show Supplier Material materials with Resistencia a la tracción of 140 MPa | dry | ISO 527-1/-2 | ||
100 °C | 70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | conditioned | ISO 179/1eA |
-30 °C | 9.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | dry | ISO 179/1eA | |
23 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 45 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 45 kJ/m² | conditioned | ISO 179/1eU |
-30 °C | 55.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 55.0 kJ/m² | dry | ISO 179/1eU | |
23 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m² | dry, conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Inflamabilidad | V-0 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
5VA | dry | 1.5 mm | IEC 60695-11-20 | |||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | 0.75 mm | UL746B | ||
Temperatura de flexión bajo carga | 205 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 205 °C | dry | ISO 75-1/-2 | 2 MPa |
Eléctrico
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Residual Current Breaker with Overload, MCCB Housings, Industrial Control Gear, Contactors, EV Charging Plugs | |
Certifications | Yellow Card Available | |
Fillers | 30% Glass Fiber |