General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 6.6 % Show Supplier Material materials with Absorción de agua of 6.6 % | dry | Sim. to ISO 62 |
Densidad | 1.38 g/cm³ Show Supplier Material materials with Densidad of 1.38 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.9 % Show Supplier Material materials with Moisture absorption of 1.9 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 3.7 % Show Supplier Material materials with Elongación of 3.7 % | dry | ISO 527-1/-2 |
3.5 % Show Supplier Material materials with Elongación of 3.5 % | dry | ISO 527-1/-2 | ||
15 % Show Supplier Material materials with Elongación of 15 % | conditioned | ISO 527-1/-2 | ||
120 °C | 100 % Show Supplier Material materials with Elongación of 100 % | dry | ISO 527-1/-2 | |
160 °C | 150 % Show Supplier Material materials with Elongación of 150 % | dry | ISO 527-1/-2 | |
180 °C | 200 % Show Supplier Material materials with Elongación of 200 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 50 MPa Show Supplier Material materials with Flexural yield strength of 50 MPa | conditioned | ISO 178 | |
120 MPa Show Supplier Material materials with Flexural yield strength of 120 MPa | dry | ISO 178 | ||
120 °C | 27 MPa Show Supplier Material materials with Flexural yield strength of 27 MPa | dry | ISO 178 | |
160 °C | 20 MPa Show Supplier Material materials with Flexural yield strength of 20 MPa | dry | ISO 178 | |
Módulo de flexión | 2.2 GPa Show Supplier Material materials with Módulo de flexión of 2.2 GPa | conditioned | ISO 178 | |
6.1 GPa Show Supplier Material materials with Módulo de flexión of 6.1 GPa | dry | ISO 178 | ||
120 °C | 1.1 GPa Show Supplier Material materials with Módulo de flexión of 1.1 GPa | dry | ISO 178 | |
160 °C | 0.9 GPa Show Supplier Material materials with Módulo de flexión of 0.9 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 6.3 GPa Show Supplier Material materials with Módulo elástico of 6.3 GPa | dry | ISO 527-1/-2 |
3 GPa Show Supplier Material materials with Módulo elástico of 3 GPa | conditioned | ISO 527-1/-2 | ||
6.1 GPa Show Supplier Material materials with Módulo elástico of 6.1 GPa | dry | ISO 527-1/-2 | ||
40 °C | 5.5 GPa Show Supplier Material materials with Módulo elástico of 5.5 GPa | dry | ISO 527-1/-2 | |
120 °C | 0.98 GPa Show Supplier Material materials with Módulo elástico of 0.98 GPa | dry | ISO 527-1/-2 | |
160 °C | 0.72 GPa Show Supplier Material materials with Módulo elástico of 0.72 GPa | dry | ISO 527-1/-2 | |
180 °C | 0.67 GPa Show Supplier Material materials with Módulo elástico of 0.67 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | dry | ISO 527-1/-2 |
40 MPa Show Supplier Material materials with Resistencia a la tracción of 40 MPa | conditioned | ISO 527-1/-2 | ||
75 MPa Show Supplier Material materials with Resistencia a la tracción of 75 MPa | dry | ISO 527-1/-2 | ||
120 °C | 25 MPa Show Supplier Material materials with Resistencia a la tracción of 25 MPa | dry | ISO 527-1/-2 | |
160 °C | 22 MPa Show Supplier Material materials with Resistencia a la tracción of 22 MPa | dry | ISO 527-1/-2 | |
180 °C | 18 MPa Show Supplier Material materials with Resistencia a la tracción of 18 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 2 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 2 kJ/m² | dry | ISO 179/1eA |
-30 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | dry | ISO 179/1eA | |
23 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 40 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 40 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 40 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 40 kJ/m² | dry | ISO 179/1eU | |
23 °C | 50 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 50 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 4e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
4e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Difusividad térmica | 1.14e-07 mm²/s Show Supplier Material materials with Difusividad térmica of 1.14e-07 mm²/s | dry | - | |||
Inflamabilidad | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | UL746B | 0.71 mm | ||
Relative temperature index, mechanical impact | 100 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 100 °C | dry | UL746B | 0.71 mm | ||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | UL746B | 0.71 mm | ||
Temperatura de flexión bajo carga | 135 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 135 °C | dry | ISO 75-1/-2 | 2 MPa | ||
205 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 205 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3 [-] Show Supplier Material materials with Constante dieléctrica of 3 [-] | dry | IEC 62631-2-1 | 1MHz |
3.2 [-] Show Supplier Material materials with Constante dieléctrica of 3.2 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.5 [-] Show Supplier Material materials with Constante dieléctrica of 4.5 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
15 [-] Show Supplier Material materials with Constante dieléctrica of 15 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 50 [-] Show Supplier Material materials with Factor de disipación of 50 [-] | dry | IEC 62631-2-1 | 100Hz |
130 [-] Show Supplier Material materials with Factor de disipación of 130 [-] | dry | IEC 62631-2-1 | 1MHz | |
1100 [-] Show Supplier Material materials with Factor de disipación of 1100 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3500 [-] Show Supplier Material materials with Factor de disipación of 3500 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Rigidez dieléctrica | 25 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 25 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | dry | IEC 60243-1 | ||
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | ||
Índice de seguimiento comparativo | 500 V Show Supplier Material materials with Índice de seguimiento comparativo of 500 V | dry, conditioned | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.69 % Show Supplier Material materials with Contracción of 0.69 % | dry | ISO 294-4 | Normal |
0.79 % Show Supplier Material materials with Contracción of 0.79 % | dry | ISO 294-4 | Parallel | |
Density of melt | 1160 g/cm³ Show Supplier Material materials with Density of melt of 1160 g/cm³ | dry | - | |
Specific heat capacity melt | 2450 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2450 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.32 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.32 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Pulley covers | |
Certifications | Yellow Card Available | |
Fillers | 30% Mineral Powder |