General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 70 % Show Supplier Material materials with Bio-based content of 70 % | dry | ASTM D6866-12 Method B |
Densidad | 1.09 g/cm³ Show Supplier Material materials with Densidad of 1.09 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 16 % Show Supplier Material materials with Elongación of 16 % | dry | ISO 527-1/-2 | |
50 % Show Supplier Material materials with Elongación of 50 % | conditioned | ISO 527-1/-2 | ||
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | dry | ISO 527-1/-2 | |
16 % Show Supplier Material materials with Elongation at yield of 16 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 55.0 MPa Show Supplier Material materials with Flexural yield strength of 55.0 MPa | conditioned | ISO 178 | |
115 MPa Show Supplier Material materials with Flexural yield strength of 115 MPa | dry | ISO 178 | ||
Módulo de flexión | 1.4 GPa Show Supplier Material materials with Módulo de flexión of 1.4 GPa | conditioned | ISO 178 | |
2.9 GPa Show Supplier Material materials with Módulo de flexión of 2.9 GPa | dry | ISO 178 | ||
Módulo elástico | 1.7 GPa Show Supplier Material materials with Módulo elástico of 1.7 GPa | conditioned | ISO 527-1/-2 | |
3.1 GPa Show Supplier Material materials with Módulo elástico of 3.1 GPa | dry | ISO 527-1/-2 | ||
120 °C | 0.75 GPa Show Supplier Material materials with Módulo elástico of 0.75 GPa | dry | ISO 527-1/-2 | |
160 °C | 0.54 GPa Show Supplier Material materials with Módulo elástico of 0.54 GPa | dry | ISO 527-1/-2 | |
180 °C | 0.4 GPa Show Supplier Material materials with Módulo elástico of 0.4 GPa | dry | ISO 527-1/-2 | |
200 °C | 0.3 GPa Show Supplier Material materials with Módulo elástico of 0.3 GPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | dry | ISO 179/1eA |
23 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13 kJ/m² | conditioned | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 7e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
9e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Temperatura de flexión bajo carga | 77 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 77 °C | dry | ISO 75-1/-2 | 2 MPa | |
175 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 175 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 250 °C Show Supplier Material materials with Temperatura de fusión of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 1.2 % Show Supplier Material materials with Contracción of 1.2 % | dry | ISO 294-4 | Parallel |
1.3 % Show Supplier Material materials with Contracción of 1.3 % | dry | ISO 294-4 | Normal | |
Density of melt | 0.9 g/cm³ Show Supplier Material materials with Density of melt of 0.9 g/cm³ | dry | - | |
Viscosity number | 150 cm³/gr Show Supplier Material materials with Viscosity number of 150 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact, Yellow Card Available |