General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.37 g/cm³ Show Supplier Material materials with Densidad of 1.37 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2.6 % Show Supplier Material materials with Elongación of 2.6 % | dry | ISO 527-1/-2 | |
4 % Show Supplier Material materials with Elongación of 4 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 200 MPa Show Supplier Material materials with Flexural yield strength of 200 MPa | conditioned | ISO 178 | |
267 MPa Show Supplier Material materials with Flexural yield strength of 267 MPa | dry | ISO 178 | ||
Módulo de flexión | 6.5 GPa Show Supplier Material materials with Módulo de flexión of 6.5 GPa | conditioned | ISO 178 | |
8.3 GPa Show Supplier Material materials with Módulo de flexión of 8.3 GPa | dry | ISO 178 | ||
Módulo elástico | 6.5 GPa Show Supplier Material materials with Módulo elástico of 6.5 GPa | conditioned | ISO 527-1/-2 | |
9.7 GPa Show Supplier Material materials with Módulo elástico of 9.7 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 130 MPa Show Supplier Material materials with Resistencia a la tracción of 130 MPa | conditioned | ISO 527-1/-2 | |
170 MPa Show Supplier Material materials with Resistencia a la tracción of 170 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 11 kJ/m² | dry | ISO 179/1eA |
23 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 80 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 80 kJ/m² | conditioned | ISO 179/1eU |
23 °C | 110 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 110 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | 0.75 mm | UL746B | ||
Temperatura de flexión bajo carga | 244 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 244 °C | dry | ISO 75-1/-2 | 2 MPa | ||
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
Factor de disipación | 190 [-] Show Supplier Material materials with Factor de disipación of 190 [-] | dry | IEC 62631-2-1 | 1MHz |
Rigidez dieléctrica | 26 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 26 kV/mm | dry | IEC 60243-1 | |
Surface resistivity | 4e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 4e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 550 V Show Supplier Material materials with Índice de seguimiento comparativo of 550 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | dry | Sim. to ISO 294-4 | Parallel | |
1.3 % Show Supplier Material materials with Contracción of 1.3 % | dry | Sim. to ISO 294-4 | Normal | ||
Velocidad de flujo de la masa derretida | 280 °C | 19 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 19 g/10min | dry | ISO 1133 | |
Velocidad de flujo del volumen derretido | 280 °C | 15 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 15 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |