General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.13 g/cm³ Show Supplier Material materials with Densidad of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.8 % Show Supplier Material materials with Moisture absorption of 2.8 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongation at yield | 4.2 % Show Supplier Material materials with Elongation at yield of 4.2 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 107 MPa Show Supplier Material materials with Flexural yield strength of 107 MPa | dry | ISO 178 | |
Módulo de flexión | 2.6 GPa Show Supplier Material materials with Módulo de flexión of 2.6 GPa | dry | ISO 178 | |
Módulo elástico | 2.7 GPa Show Supplier Material materials with Módulo elástico of 2.7 GPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 2.6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 2.6 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | dry | 0.71 mm | UL746B | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | 0.71 mm | UL746B | ||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | dry | 0.71 mm | UL746B | ||
Temperatura de flexión bajo carga | 62 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 62 °C | dry | ISO 75-1/-2 | 2 MPa | ||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 230 °C | 10 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 10 cm³/10min | dry | ISO 1133 |
Viscosity number | 183 cm³/gr Show Supplier Material materials with Viscosity number of 183 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact, Yellow Card Available |