General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.6 % Show Supplier Material materials with Absorción de agua of 0.6 % | dry | Sim. to ISO 62 |
Densidad | 1.26 g/cm³ Show Supplier Material materials with Densidad of 1.26 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.25 % Show Supplier Material materials with Moisture absorption of 0.25 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 55.0 [-] Show Supplier Material materials with Dureza Shore D of 55.0 [-] | dry | ISO 868 | 3s | |
55.0 [-] Show Supplier Material materials with Dureza Shore D of 55.0 [-] | dry | ISO 868 | 15s | ||
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | ||
300 % Show Supplier Material materials with Elongación of 300 % | dry | ISO 527-1/-2 | |||
Elongation at yield | 22 % Show Supplier Material materials with Elongation at yield of 22 % | dry | ISO 527-1/-2 | ||
Módulo elástico | 0.2 GPa Show Supplier Material materials with Módulo elástico of 0.2 GPa | dry | ISO 527-1/-2 | ||
Resistencia a desgarros | 165 kN/m Show Supplier Material materials with Resistencia a desgarros of 165 kN/m | dry | ISO 34-1; Method B | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 6 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1.6e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.6e-06 1/K | dry | ISO 11359-1/-2 | Parallel | ||
Inflamabilidad | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 160 °C Show Supplier Material materials with Relative temperature index, electrical of 160 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 120 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 150 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C | dry | UL746B | 0.75 mm | ||
Temperatura de flexión bajo carga | 80 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 80 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 200 °C Show Supplier Material materials with Temperatura de fusión of 200 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de reblandecimiento Vicat | 85 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 85 °C | dry | ISO 306 | 50°C/h 50N |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.35 % Show Supplier Material materials with Contracción of 1.35 % | dry | ISO 294-4 | Normal | |
1.45 % Show Supplier Material materials with Contracción of 1.45 % | dry | ISO 294-4 | Parallel | ||
Velocidad de flujo de la masa derretida | 230 °C | 14.0 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 14.0 g/10min | dry | ISO 1133 | |
Velocidad de flujo del volumen derretido | 230 °C | 13.8 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 13.8 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Wire and Cable Insulation, Convoluted Tubes, Support Springs | |
Certifications | Yellow Card Available |