General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 7 % Show Supplier Material materials with Absorción de agua of 7 % | dry | Sim. to ISO 62 |
Densidad | 1.16 g/cm³ Show Supplier Material materials with Densidad of 1.16 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.4 % Show Supplier Material materials with Moisture absorption of 0.4 % | dry | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 32 [-] Show Supplier Material materials with Dureza Shore D of 32 [-] | dry | ISO 868 | 3s |
Elongación | 200 % Show Supplier Material materials with Elongación of 200 % | dry | ISO 527-1/-2 | |
Módulo elástico | 0.06 GPa Show Supplier Material materials with Módulo elástico of 0.06 GPa | dry | ISO 527-1/-2 | |
Resistencia a desgarros | 80 kN/m Show Supplier Material materials with Resistencia a desgarros of 80 kN/m | dry | ISO 34-1; Method B | |
Resistencia a la tracción | 13.1 MPa Show Supplier Material materials with Resistencia a la tracción of 13.1 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Coeficiente de dilatación térmica | 1.5e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.5e-06 1/K | dry | ISO 11359-1/-2 | Parallel |
1.5e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.5e-06 1/K | dry | ISO 11359-1/-2 | Normal | |
Temperatura de fusión | 212 °C Show Supplier Material materials with Temperatura de fusión of 212 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4.4 [-] Show Supplier Material materials with Constante dieléctrica of 4.4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.7 [-] Show Supplier Material materials with Constante dieléctrica of 4.7 [-] | dry | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 310 [-] Show Supplier Material materials with Factor de disipación of 310 [-] | dry | IEC 62631-2-1 | 100Hz |
810 [-] Show Supplier Material materials with Factor de disipación of 810 [-] | dry | IEC 62631-2-1 | 1MHz | |
Rigidez dieléctrica | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | dry | IEC 60243-1 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 230 °C | 13.5 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 13.5 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Roofing membranes, Breathable Outdoor clothing, Medical gowns | |
Certifications | Food Contact |