General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.65 % Show Supplier Material materials with Absorción de agua of 0.65 % | dry | Sim. to ISO 62 |
Densidad | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.2 % Show Supplier Material materials with Moisture absorption of 0.2 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 54 [-] Show Supplier Material materials with Dureza Shore D of 54 [-] | dry | ISO 868 | 3s | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | ||
300 % Show Supplier Material materials with Elongación of 300 % | dry | ISO 527-1/-2 | |||
Elongation at yield | 33 % Show Supplier Material materials with Elongation at yield of 33 % | dry | ISO 527-1/-2 | ||
Módulo elástico | 0.17 GPa Show Supplier Material materials with Módulo elástico of 0.17 GPa | dry | ISO 527-1/-2 | ||
Resistencia a desgarros | 150 kN/m Show Supplier Material materials with Resistencia a desgarros of 150 kN/m | dry | ISO 34-1; Method B | ||
Resistencia a la tracción | 32 MPa Show Supplier Material materials with Resistencia a la tracción of 32 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 25 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 25 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-06 1/K | dry | ISO 11359-1/-2 | Parallel | ||
2e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-06 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | UL746B | 2 mm | ||
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | UL746B | 2 mm | ||
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | UL746B | 2 mm | ||
Temperatura de flexión bajo carga | 110 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 110 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 204 °C Show Supplier Material materials with Temperatura de fusión of 204 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de reblandecimiento Vicat | 90 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 90 °C | dry | ISO 306 | 50°C/h 50N | ||
Temperatura de transición del vidrio | -64 °C Show Supplier Material materials with Temperatura de transición del vidrio of -64 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.4 [-] Show Supplier Material materials with Constante dieléctrica of 4.4 [-] | dry | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 400 [-] Show Supplier Material materials with Factor de disipación of 400 [-] | dry | IEC 62631-2-1 | 1MHz |
Rigidez dieléctrica | 21 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 21 kV/mm | dry | IEC 60243-1 | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.55 % Show Supplier Material materials with Contracción of 1.55 % | dry | Sim. to ISO 294-4 | Parallel | |
1.55 % Show Supplier Material materials with Contracción of 1.55 % | dry | Sim. to ISO 294-4 | Normal | ||
Velocidad de flujo del volumen derretido | 230 °C | 23 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 23 cm³/10min | dry | ISO 1133 |
Technological properties
Property |
---|