General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.8 % Show Supplier Material materials with Absorción de agua of 0.8 % | dry | Sim. to ISO 62 |
Densidad | 1.09 g/cm³ Show Supplier Material materials with Densidad of 1.09 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore A | 82 [-] Show Supplier Material materials with Dureza Shore A of 82 [-] | dry | ISO 868 | 3s |
Elongación | 900 % Show Supplier Material materials with Elongación of 900 % | dry | ISO 527-1/-2 | |
Módulo elástico | 0.02 GPa Show Supplier Material materials with Módulo elástico of 0.02 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 12 MPa Show Supplier Material materials with Resistencia a la tracción of 12 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 180 °C Show Supplier Material materials with Temperatura de fusión of 180 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de transición del vidrio | -80 °C Show Supplier Material materials with Temperatura de transición del vidrio of -80 °C | dry | ISO 11357-1/-2 | 10°C/min |
-74 °C Show Supplier Material materials with Temperatura de transición del vidrio of -74 °C | dry | ASTM D5026/D7028 | DMTA (tan d) |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Density of melt | 905 g/cm³ Show Supplier Material materials with Density of melt of 905 g/cm³ | dry | - | |
Velocidad de flujo del volumen derretido | 230 °C | 55.0 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 55.0 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Phone case |