General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 3.3 % Show Supplier Material materials with Absorción de agua of 3.3 % | dry | Sim. to ISO 62 |
Densidad | 1.58 g/cm³ Show Supplier Material materials with Densidad of 1.58 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.3 % Show Supplier Material materials with Moisture absorption of 1.3 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Elongación | 1.6 % Show Supplier Material materials with Elongación of 1.6 % | dry, conditioned | ISO 527-1/-2 | |||
1.6 % Show Supplier Material materials with Elongación of 1.6 % | dry, conditioned | ISO 527-1/-2 | 1 mm | |||
120 °C | 3 % Show Supplier Material materials with Elongación of 3 % | dry | ISO 527-1/-2 | |||
160 °C | 5 % Show Supplier Material materials with Elongación of 5 % | dry | ISO 527-1/-2 | |||
Flexural yield strength | 150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | conditioned | ISO 178 | |||
165 MPa Show Supplier Material materials with Flexural yield strength of 165 MPa | dry | ISO 178 | ||||
120 °C | 90 MPa Show Supplier Material materials with Flexural yield strength of 90 MPa | dry | ISO 178 | |||
160 °C | 60 MPa Show Supplier Material materials with Flexural yield strength of 60 MPa | dry | ISO 178 | |||
Módulo de flexión | 11.3 GPa Show Supplier Material materials with Módulo de flexión of 11.3 GPa | dry | ISO 178 | |||
11.6 GPa Show Supplier Material materials with Módulo de flexión of 11.6 GPa | conditioned | ISO 178 | ||||
120 °C | 6.4 GPa Show Supplier Material materials with Módulo de flexión of 6.4 GPa | dry | ISO 178 | |||
160 °C | 3.6 GPa Show Supplier Material materials with Módulo de flexión of 3.6 GPa | dry | ISO 178 | |||
Módulo elástico | 11.5 GPa Show Supplier Material materials with Módulo elástico of 11.5 GPa | dry | ISO 527-1/-2 | |||
11.5 GPa Show Supplier Material materials with Módulo elástico of 11.5 GPa | dry | ISO 527-1/-2 | 1 mm | |||
11.8 GPa Show Supplier Material materials with Módulo elástico of 11.8 GPa | conditioned | ISO 527-1/-2 | ||||
11.8 GPa Show Supplier Material materials with Módulo elástico of 11.8 GPa | conditioned | ISO 527-1/-2 | ||||
120 °C | 6 GPa Show Supplier Material materials with Módulo elástico of 6 GPa | dry | ISO 527-1/-2 | |||
160 °C | 3.1 GPa Show Supplier Material materials with Módulo elástico of 3.1 GPa | dry | ISO 527-1/-2 | |||
Resistencia a la tracción | 100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | conditioned | ISO 527-1/-2 | |||
100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | conditioned | ISO 527-1/-2 | at low thickness | |||
110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | dry | ISO 527-1/-2 | ||||
110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | dry | ISO 527-1/-2 | 1 mm | at low thickness | ||
120 °C | 57.0 MPa Show Supplier Material materials with Resistencia a la tracción of 57.0 MPa | dry | ISO 527-1/-2 | |||
160 °C | 37 MPa Show Supplier Material materials with Resistencia a la tracción of 37 MPa | dry | ISO 527-1/-2 | |||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | dry, conditioned | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 26 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 26 kJ/m² | dry, conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 3e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3e-07 1/K | dry | ASTM D696 | Parallel | |
4e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4e-07 1/K | dry | ASTM D696 | Normal | ||
Temperatura de flexión bajo carga | 290 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 290 °C | dry | ISO 75-1/-2 | 2 MPa | |
310 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 310 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 325 °C Show Supplier Material materials with Temperatura de fusión of 325 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 125 °C Show Supplier Material materials with Temperatura de transición del vidrio of 125 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4.06 [-] Show Supplier Material materials with Constante dieléctrica of 4.06 [-] | dry | IEC 60250 | 5GHz |
4.12 [-] Show Supplier Material materials with Constante dieléctrica of 4.12 [-] | conditioned | IEC 60250 | 5GHz | |
4.13 [-] Show Supplier Material materials with Constante dieléctrica of 4.13 [-] | dry | IEC 60250 | 1GHz | |
4.23 [-] Show Supplier Material materials with Constante dieléctrica of 4.23 [-] | conditioned | IEC 60250 | 1GHz | |
Factor de disipación | 165 [-] Show Supplier Material materials with Factor de disipación of 165 [-] | dry | IEC 60250 | 5GHz |
182 [-] Show Supplier Material materials with Factor de disipación of 182 [-] | conditioned | IEC 60250 | 5GHz | |
210 [-] Show Supplier Material materials with Factor de disipación of 210 [-] | dry | IEC 60250 | 1GHz | |
217 [-] Show Supplier Material materials with Factor de disipación of 217 [-] | conditioned | IEC 60250 | 1GHz | |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry, conditioned | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 400 V Show Supplier Material materials with Índice de seguimiento comparativo of 400 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 30% Glass Fiber |