Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.37 g/cm³ Show Supplier Material materials with Densidad of 1.37 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2.7 % Show Supplier Material materials with Elongación of 2.7 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 170 MPa Show Supplier Material materials with Flexural yield strength of 170 MPa | dry | ISO 178 | |
Módulo de flexión | 7 GPa Show Supplier Material materials with Módulo de flexión of 7 GPa | dry | ISO 178 | |
Módulo elástico | 7.7 GPa Show Supplier Material materials with Módulo elástico of 7.7 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 115 MPa Show Supplier Material materials with Resistencia a la tracción of 115 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 6.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6.5 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 276 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 276 °C | dry | ISO 75-1/-2 | 2 MPa | |
284 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 284 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.5 [-] Show Supplier Material materials with Constante dieléctrica of 3.5 [-] | dry | IEC 60250 | 1GHz |
Factor de disipación | 100 [-] Show Supplier Material materials with Factor de disipación of 100 [-] | dry | IEC 60250 | 1GHz |
Rigidez dieléctrica | 30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | dry | IEC 60243-1 | |
Índice de seguimiento comparativo | 575 V Show Supplier Material materials with Índice de seguimiento comparativo of 575 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | dry | ISO 294-4 | Parallel |
1.5 % Show Supplier Material materials with Contracción of 1.5 % | dry | ISO 294-4 | Normal | |
Spiral flow length | 165 | dry | - | 1.0 mm 800 bar |
180 | dry | - | 1.0 mm 900 bar | |
200 | dry | - | 1.0 mm 1000 bar |
Technological properties
Property | ||
---|---|---|
Application areas | USB-C Connectors | |
Certifications | Yellow Card Available | |
Fillers | 20% Glass Fiber |