General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.17 g/cm³ Show Supplier Material materials with Densidad of 1.17 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard |
---|---|---|---|
Elongación | 3 % Show Supplier Material materials with Elongación of 3 % | dry | ISO 527-1/-2 |
Elongation at yield | 2.8 % Show Supplier Material materials with Elongation at yield of 2.8 % | dry | ISO 527-1/-2 |
Módulo elástico | 7.6 GPa Show Supplier Material materials with Módulo elástico of 7.6 GPa | dry | ISO 527-1/-2 |
Resistencia a la tracción | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 153 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 153 °C | dry | ISO 75-1/-2 | 2 MPa | |
184 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 184 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 200 °C Show Supplier Material materials with Temperatura de fusión of 200 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 58.0 °C Show Supplier Material materials with Temperatura de transición del vidrio of 58.0 °C | dry | ISO 11357-1/-2 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Fillers | 10% Carbon Fiber |