General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 1.6 % Show Supplier Material materials with Absorción de agua of 1.6 % | dry | ISO 62 | at 23°C after 24h |
5.8 % Show Supplier Material materials with Absorción de agua of 5.8 % | dry | Sim. to ISO 62 | ||
Densidad | 1.68 g/cm³ Show Supplier Material materials with Densidad of 1.68 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|---|
Elongación | 1.8 % Show Supplier Material materials with Elongación of 1.8 % | dry | 1 mm | ISO 527-1/-2 | ||
1.9 % Show Supplier Material materials with Elongación of 1.9 % | dry | 1 mm | ISO 527-1/-2 | |||
2.8 % Show Supplier Material materials with Elongación of 2.8 % | conditioned | ISO 527-1/-2 | ||||
Flexural yield strength | 165 MPa Show Supplier Material materials with Flexural yield strength of 165 MPa | conditioned | ISO 178 | |||
240 MPa Show Supplier Material materials with Flexural yield strength of 240 MPa | dry | ISO 178 | ||||
Módulo de flexión | 6.8 GPa Show Supplier Material materials with Módulo de flexión of 6.8 GPa | conditioned | ISO 178 | |||
11 GPa Show Supplier Material materials with Módulo de flexión of 11 GPa | dry | ISO 178 | ||||
Módulo elástico | 7.5 GPa Show Supplier Material materials with Módulo elástico of 7.5 GPa | conditioned | ISO 527-1/-2 | |||
12 GPa Show Supplier Material materials with Módulo elástico of 12 GPa | dry | 1 mm | ISO 527-1/-2 | |||
13 GPa Show Supplier Material materials with Módulo elástico of 13 GPa | dry | 1 mm | ISO 527-1/-2 | |||
Resistencia a la tracción | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | conditioned | ISO 527-1/-2 | |||
170 MPa Show Supplier Material materials with Resistencia a la tracción of 170 MPa | dry | 1 mm | ISO 527-1/-2 | |||
180 MPa Show Supplier Material materials with Resistencia a la tracción of 180 MPa | dry | 1 mm | ISO 527-1/-2 | at low thickness | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | dry, conditioned | ISO 179/1eA | ||
23 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13 kJ/m² | dry, conditioned | ISO 179/1eA | |||
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 40 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 40 kJ/m² | dry, conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
4.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Difusividad térmica | 1.01e-07 mm²/s Show Supplier Material materials with Difusividad térmica of 1.01e-07 mm²/s | dry | - | |||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 3 mm | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.75 mm | |||
Glow Wire Ignition Temperature | 850 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 850 °C | dry | IEC 60695-2-13 | 2 mm | ||
960 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 960 °C | dry | IEC 60695-2-13 | 3 mm | |||
Inflamabilidad | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.35 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.35 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.35 mm | ||
Temperatura de flexión bajo carga | 290 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 290 °C | dry | ISO 75-1/-2 | 2 MPa | ||
290 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 290 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de reblandecimiento Vicat | 290 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 290 °C | dry | ISO 306 | 50°C/h 50N | ||
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.3 [-] Show Supplier Material materials with Constante dieléctrica of 4.3 [-] | dry | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 60 [-] Show Supplier Material materials with Factor de disipación of 60 [-] | dry | IEC 62631-2-1 | 100Hz |
160 [-] Show Supplier Material materials with Factor de disipación of 160 [-] | dry | IEC 62631-2-1 | 1MHz | |
Rigidez dieléctrica | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | dry | IEC 60243-1 | ||
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+08 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+08 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | ||
Índice de seguimiento comparativo | 225 V Show Supplier Material materials with Índice de seguimiento comparativo of 225 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | dry | Sim. to ISO 294-4 | Parallel |
1.1 % Show Supplier Material materials with Contracción of 1.1 % | dry | Sim. to ISO 294-4 | Normal | |
Density of melt | 1450 g/cm³ Show Supplier Material materials with Density of melt of 1450 g/cm³ | dry | - | |
Specific heat capacity melt | 1750 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1750 J/(kg·K) | dry | - | |
Spiral flow length | 112 | dry | - | 0.5mm 1200 bar |
132 | dry | - | 0.5mm 1600 bar | |
151 | dry | - | 0.5mm 2000 bar | |
Thermal conductivity of melt | 0.258 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.258 W/(m·K) | dry | - | |
Viscosity number | 66 cm³/gr Show Supplier Material materials with Viscosity number of 66 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 30% Glass Fiber |