General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 5.6 % Show Supplier Material materials with Absorción de agua of 5.6 % | dry | Sim. to ISO 62 |
Densidad | 1.44 g/cm³ Show Supplier Material materials with Densidad of 1.44 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 3.2 % Show Supplier Material materials with Elongación of 3.2 % | dry | ISO 527-1/-2 | |
20 % Show Supplier Material materials with Elongación of 20 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 80 MPa Show Supplier Material materials with Flexural yield strength of 80 MPa | conditioned | ISO 178 | |
160 MPa Show Supplier Material materials with Flexural yield strength of 160 MPa | dry | ISO 178 | ||
Módulo de flexión | 3.7 GPa Show Supplier Material materials with Módulo de flexión of 3.7 GPa | conditioned | ISO 178 | |
7.5 GPa Show Supplier Material materials with Módulo de flexión of 7.5 GPa | dry | ISO 178 | ||
Módulo elástico | 3.5 GPa Show Supplier Material materials with Módulo elástico of 3.5 GPa | conditioned | ISO 527-1/-2 | |
7.8 GPa Show Supplier Material materials with Módulo elástico of 7.8 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 50 MPa Show Supplier Material materials with Resistencia a la tracción of 50 MPa | conditioned | ISO 527-1/-2 | |
95 MPa Show Supplier Material materials with Resistencia a la tracción of 95 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | dry | ISO 179/1eA | |
23 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 40 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 40 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 43 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 43 kJ/m² | dry | ISO 179/1eU | |
23 °C | 80 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 80 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 2 mm | IEC 60695-2-12 | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 0.75 mm | IEC 60695-2-12 | |||
Glow Wire Ignition Temperature | 750 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 750 °C | dry | 2 mm | IEC 60695-2-13 | ||
775 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 775 °C | dry | 0.75 mm | IEC 60695-2-13 | |||
Inflamabilidad | V-2 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | dry | 0.75 mm | UL746B | ||
Temperatura de flexión bajo carga | 180 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 180 °C | dry | ISO 75-1/-2 | 2 MPa | ||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Índice de seguimiento comparativo | 525 V Show Supplier Material materials with Índice de seguimiento comparativo of 525 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Residual Current device, Contactors, Switch Base | |
Certifications | Yellow Card Available | |
Fillers | 30% Glass Fiber |