General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.2 % Show Supplier Material materials with Absorción de agua of 0.2 % | dry | Sim. to ISO 62 |
Densidad | 1.13 g/cm³ Show Supplier Material materials with Densidad of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.65 % Show Supplier Material materials with Moisture absorption of 0.65 % | dry | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore A | 88 [-] Show Supplier Material materials with Dureza Shore A of 88 [-] | dry | ISO 868 | 3s |
Elongación | 440 % Show Supplier Material materials with Elongación of 440 % | dry | ISO 527-1/-2 | |
Módulo elástico | 0.06 GPa Show Supplier Material materials with Módulo elástico of 0.06 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 10.6 MPa Show Supplier Material materials with Resistencia a la tracción of 10.6 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 195 °C Show Supplier Material materials with Temperatura de fusión of 195 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de transición del vidrio | -70 °C Show Supplier Material materials with Temperatura de transición del vidrio of -70 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 19.8 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 19.8 kV/mm | dry | IEC 60243-1 |
Volume resistivity | 8.3e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 8.3e+10 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 230 °C | 4.3 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 4.3 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | AC Cables, DC Cables | |
Certifications | Yellow Card Available |