General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 6 % Show Supplier Material materials with Absorción de agua of 6 % | dry | Sim. to ISO 62 |
Densidad | 1.4 g/cm³ Show Supplier Material materials with Densidad of 1.4 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 3 % Show Supplier Material materials with Elongación of 3 % | dry | ISO 527-1/-2 | |
5 % Show Supplier Material materials with Elongación of 5 % | conditioned | ISO 527-1/-2 | ||
Módulo de flexión | 9.2 GPa Show Supplier Material materials with Módulo de flexión of 9.2 GPa | dry | ISO 178 | |
Módulo elástico | 7.5 GPa Show Supplier Material materials with Módulo elástico of 7.5 GPa | conditioned | ISO 527-1/-2 | |
10.5 GPa Show Supplier Material materials with Módulo elástico of 10.5 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 140 MPa Show Supplier Material materials with Resistencia a la tracción of 140 MPa | conditioned | ISO 527-1/-2 | |
185 MPa Show Supplier Material materials with Resistencia a la tracción of 185 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | dry | ISO 179/1eA |
-30 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA | |
23 °C | 20 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 20 kJ/m² | conditioned | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
7e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Inflamabilidad | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 2 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 2 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 2 mm | ||
Temperatura de flexión bajo carga | 250 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 250 °C | dry | ISO 75-1/-2 | 2 MPa | ||
260 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 260 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de transición del vidrio | 60 °C Show Supplier Material materials with Temperatura de transición del vidrio of 60 °C | dry | ISO 11357-1/-2 | 10°C/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 32% Glass Fiber and MoS2 |