General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.27 g/cm³ Show Supplier Material materials with Densidad of 1.27 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 61 [-] Show Supplier Material materials with Dureza Shore D of 61 [-] | dry | ISO 868 | 3s | |
Elongación | 290 % Show Supplier Material materials with Elongación of 290 % | dry | ISO 527-1/-2 | ||
630 % Show Supplier Material materials with Elongación of 630 % | dry | ISO 527-1/-2 | |||
Módulo de flexión | 0.3 GPa Show Supplier Material materials with Módulo de flexión of 0.3 GPa | dry | ISO 178 | ||
120 °C | 0.1 GPa Show Supplier Material materials with Módulo de flexión of 0.1 GPa | dry | ISO 178 | ||
Módulo elástico | 0.27 GPa Show Supplier Material materials with Módulo elástico of 0.27 GPa | dry | ISO 527-1/-2 | ||
Resistencia a desgarros | 175 kN/m Show Supplier Material materials with Resistencia a desgarros of 175 kN/m | dry | ISO 34-1; Method B | ||
203 kN/m Show Supplier Material materials with Resistencia a desgarros of 203 kN/m | dry | ISO 34-1; Method B | |||
Resistencia a la tracción | 26 MPa Show Supplier Material materials with Resistencia a la tracción of 26 MPa | dry | ISO 527-1/-2 | ||
45 MPa Show Supplier Material materials with Resistencia a la tracción of 45 MPa | dry | ISO 527-1/-2 | Normal | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 8.7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8.7 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 206 °C Show Supplier Material materials with Temperatura de fusión of 206 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo de la masa derretida | 230 °C | 25 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 25 g/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Clean Air Inlet Ducts, Hot Charged Air Ducts |