General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.11 g/cm³ Show Supplier Material materials with Densidad of 1.11 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 33 [-] Show Supplier Material materials with Dureza Shore D of 33 [-] | dry | ISO 868 | 15s |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
300 % Show Supplier Material materials with Elongación of 300 % | dry | ISO 527-1/-2 | ||
Elongation at yield | 50 % Show Supplier Material materials with Elongation at yield of 50 % | dry | ISO 527-1/-2 | |
Módulo elástico | 0.04 GPa Show Supplier Material materials with Módulo elástico of 0.04 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 20 MPa Show Supplier Material materials with Resistencia a la tracción of 20 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 195 °C Show Supplier Material materials with Temperatura de fusión of 195 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de transición del vidrio | -73 °C Show Supplier Material materials with Temperatura de transición del vidrio of -73 °C | dry | ISO 11357-1/-2 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.5 % Show Supplier Material materials with Contracción of 1.5 % | dry | Sim. to ISO 294-4 | Parallel | |
1.5 % Show Supplier Material materials with Contracción of 1.5 % | dry | Sim. to ISO 294-4 | Normal | ||
Velocidad de flujo de la masa derretida | 230 °C | 32 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 32 g/10min | dry | ISO 1133 |
Technological properties
Property |
---|