General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 9.5 % Show Supplier Material materials with Absorción de agua of 9.5 % | dry | Sim. to ISO 62 |
Coefficient of friction, kinetic | 0.8 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.8 [-] | dry | ISO 8295 |
Densidad | 1.13 g/cm³ Show Supplier Material materials with Densidad of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.5 % Show Supplier Material materials with Moisture absorption of 2.5 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 45 % Show Supplier Material materials with Elongación of 45 % | dry | ISO 527-1/-2 | |
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-1/-2 | |
Módulo elástico | 3.1 GPa Show Supplier Material materials with Módulo elástico of 3.1 GPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 5.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5.5 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1e-06 1/K | dry | ISO 11359-1/-2 | Parallel | ||
Inflamabilidad | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 2 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 2 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 2 mm | ||
Temperatura de flexión bajo carga | 60 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 60 °C | dry | ISO 75-1/-2 | 2 MPa | ||
170 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 170 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.1 [-] Show Supplier Material materials with Constante dieléctrica of 3.1 [-] | dry | IEC 62631-2-1 | 1MHz |
3.4 [-] Show Supplier Material materials with Constante dieléctrica of 3.4 [-] | dry | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 65 [-] Show Supplier Material materials with Factor de disipación of 65 [-] | dry | IEC 62631-2-1 | 100Hz |
165 [-] Show Supplier Material materials with Factor de disipación of 165 [-] | dry | IEC 62631-2-1 | 1MHz | |
Rigidez dieléctrica | 25 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 25 kV/mm | dry | IEC 60243-1 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard |
---|---|---|---|
Viscosity number | 245 cm³/gr Show Supplier Material materials with Viscosity number of 245 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Convoluted Tubes, Timing drive systems | |
Certifications | Yellow Card Available |