EcoPaXX® is our bio-based, high-performance polyamide (PA410) that offers outstanding performance across the board, while being made mainly from tropical castor beans which don’t compete with the food chain.
EcoPaXX® belongs to the family of long-chain polyamides, which offer exceptional performance in the most demanding of environments. That includes excellent chemical resistance, low moisture absorption, combined with a very high melting point (highest of all bio-plastics) and high crystallization rate (typical for engineering plastics like PA66 and PA46).
EcoPaXX® has the lowest carbon footprint amongst common polyamides. This is because the amount of carbon dioxide emitted during the production of EcoPaXX® is offset by the amount absorbed in plant growth, and in particular by the riccinus communis – the tropical castor bean plant that makes up some 70% of EcoPaXX®. Externally certified lifecycle analysis (LCA) data is available upon request.

Datasheet URL:

EcoPaXX® Q170E-H B-MB

Los datos sobre este material han sido proporcionados por DSM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyValueConditionTesting Standard

Absorción de agua

5.8 %

Show Supplier Material materials with Absorción de agua of 5.8 %

dry

Sim. to ISO 62

Bio-based content

70 %

Show Supplier Material materials with Bio-based content of 70 %

dry

ASTM D6866-12 Method B

Densidad

1.09 g/cm³

Show Supplier Material materials with Densidad of 1.09 g/cm³

dry

ISO 1183

Moisture absorption

1.9 %

Show Supplier Material materials with Moisture absorption of 1.9 %

dry

Sim. to ISO 62

Mecánica

PropertyTemperatureValueConditionTesting Standard

Elongación

20 %

Show Supplier Material materials with Elongación of 20 %

dry

ISO 527-1/-2

50 %

Show Supplier Material materials with Elongación of 50 %

conditioned

ISO 527-1/-2

120 °C

200 %

Show Supplier Material materials with Elongación of 200 %

dry

ISO 527-1/-2

140 °C

200 %

Show Supplier Material materials with Elongación of 200 %

dry

ISO 527-1/-2

Elongation at yield

4.6 %

Show Supplier Material materials with Elongation at yield of 4.6 %

dry

ISO 527-1/-2

20 %

Show Supplier Material materials with Elongation at yield of 20 %

conditioned

ISO 527-1/-2

Módulo elástico

1.6 GPa

Show Supplier Material materials with Módulo elástico of 1.6 GPa

conditioned

ISO 527-1/-2

3.2 GPa

Show Supplier Material materials with Módulo elástico of 3.2 GPa

dry

ISO 527-1/-2

120 °C

0.6 GPa

Show Supplier Material materials with Módulo elástico of 0.6 GPa

dry

ISO 527-1/-2

140 °C

0.52 GPa

Show Supplier Material materials with Módulo elástico of 0.52 GPa

dry

ISO 527-1/-2

Resistencia a la tracción

45 MPa

Show Supplier Material materials with Resistencia a la tracción of 45 MPa

conditioned

ISO 527-1/-2

55.0 MPa

Show Supplier Material materials with Resistencia a la tracción of 55.0 MPa

dry

ISO 527-1/-2

120 °C

38 MPa

Show Supplier Material materials with Resistencia a la tracción of 38 MPa

dry

ISO 527-1/-2

140 °C

32 MPa

Show Supplier Material materials with Resistencia a la tracción of 32 MPa

dry

ISO 527-1/-2

Resistencia al choque, ensayo Charpy entallado

-30 °C

4 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m²

dry

ISO 179/1eA

-30 °C

4.5 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4.5 kJ/m²

conditioned

ISO 179/1eA

23 °C

5.5 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5.5 kJ/m²

dry

ISO 179/1eA

23 °C

12 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m²

conditioned

ISO 179/1eA

Aplicaciones térmicas

PropertyValueConditionTesting StandardPressureComment

Temperatura de flexión bajo carga

75 °C

Show Supplier Material materials with Temperatura de flexión bajo carga of 75 °C

dry

ISO 75-1/-2

2 MPa

175 °C

Show Supplier Material materials with Temperatura de flexión bajo carga of 175 °C

dry

ISO 75-1/-2

0.45 MPa

Temperatura de fusión

250 °C

Show Supplier Material materials with Temperatura de fusión of 250 °C

dry

ISO 11357-1/-3

10°C/min

Rheological Properties

PropertyTemperatureValueConditionTesting Standard

Velocidad de flujo de la masa derretida

280 °C

24 g/10min

Show Supplier Material materials with Velocidad de flujo de la masa derretida of 24 g/10min

dry

ISO 1133

Velocidad de flujo del volumen derretido

280 °C

26 cm³/10min

Show Supplier Material materials with Velocidad de flujo del volumen derretido of 26 cm³/10min

dry

ISO 1133

Viscosity number

170 cm³/gr

Show Supplier Material materials with Viscosity number of 170 cm³/gr

dry

ISO 307, 1157, 1628

Technological properties

Property