General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.63 g/cm³ Show Supplier Material materials with Densidad of 1.63 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 0.6 % Show Supplier Material materials with Elongación of 0.6 % | dry | ISO 527-1/-2 | |
Módulo elástico | 11 GPa Show Supplier Material materials with Módulo elástico of 11 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 55.0 MPa Show Supplier Material materials with Resistencia a la tracción of 55.0 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 1.6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 1.6 kJ/m² | dry | ISO 179/1eA |
23 °C | 2 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 2 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 10 kJ/m² | dry | ISO 179/1eU |
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 10 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
2.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Conductividad térmica | 1 W/(m·K) Show Supplier Material materials with Conductividad térmica of 1 W/(m·K) | dry | ASTM E1461 | through plane | |
5 W/(m·K) Show Supplier Material materials with Conductividad térmica of 5 W/(m·K) | dry | ASTM E1461 | in plane | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.75 mm | |
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 3 mm | ||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | dry | IEC 60695-2-13 | 0.75 mm | |
825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | dry | IEC 60695-2-13 | 3 mm | ||
Inflamabilidad | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes |
5VA | dry | IEC 60695-11-20 | 1.6 mm |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.89 [-] Show Supplier Material materials with Constante dieléctrica of 3.89 [-] | dry | IEC 60250 | 5GHz |
3.89 [-] Show Supplier Material materials with Constante dieléctrica of 3.89 [-] | dry | IEC 60250 | 10GHz | |
Factor de disipación | 59 [-] Show Supplier Material materials with Factor de disipación of 59 [-] | dry | IEC 60250 | 10GHz |
60 [-] Show Supplier Material materials with Factor de disipación of 60 [-] | dry | IEC 60250 | 5GHz | |
Índice de seguimiento comparativo | 575 V Show Supplier Material materials with Índice de seguimiento comparativo of 575 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |