General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.77 g/cm³ Show Supplier Material materials with Densidad of 1.77 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.1 % Show Supplier Material materials with Moisture absorption of 1.1 % | dry | Sim. to ISO 62 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 320 °C Show Supplier Material materials with Temperatura de fusión of 320 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de transición del vidrio | 145 °C Show Supplier Material materials with Temperatura de transición del vidrio of 145 °C | dry | ASTM D5026/D7028 | DMTA (tan d) |
Technological properties
Property | ||
---|---|---|
Fillers | 60% Glass Fiber |