General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.35 % Show Supplier Material materials with Absorción de agua of 0.35 % | dry | Sim. to ISO 62 |
Densidad | 1.37 g/cm³ Show Supplier Material materials with Densidad of 1.37 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.16 % Show Supplier Material materials with Moisture absorption of 0.16 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 4 % Show Supplier Material materials with Elongación of 4 % | dry | ISO 527-1/-2 | |
Módulo elástico | 4.6 GPa Show Supplier Material materials with Módulo elástico of 4.6 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 90 MPa Show Supplier Material materials with Resistencia a la tracción of 90 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA |
23 °C | 3.9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3.9 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 30 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 30 kJ/m² | dry | ISO 179/1eU |
23 °C | 34 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 34 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Coeficiente de dilatación térmica | 6e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6e-07 1/K | dry | ISO 11359-1/-2 | Parallel |
8e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8e-07 1/K | dry | ISO 11359-1/-2 | Normal | |
Temperatura de fusión | 225 °C Show Supplier Material materials with Temperatura de fusión of 225 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 0.85 % Show Supplier Material materials with Contracción of 0.85 % | dry | Sim. to ISO 294-4 | Parallel | |
1.5 % Show Supplier Material materials with Contracción of 1.5 % | dry | Sim. to ISO 294-4 | Normal | ||
Velocidad de flujo del volumen derretido | 250 °C | 21 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 21 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Bezels and AFL Frames, Fuse Holders, E-Boxes | |
Fillers | 10% Glass Fiber |