General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 3 % Show Supplier Material materials with Absorción de agua of 3 % | dry | ISO 62 | at 23°C after 24h |
11 % Show Supplier Material materials with Absorción de agua of 11 % | dry | Sim. to ISO 62 | ||
Densidad | 1.1 g/cm³ Show Supplier Material materials with Densidad of 1.1 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2.95 % Show Supplier Material materials with Moisture absorption of 2.95 % | dry | Sim. to ISO 62 | |
Índice límite de óxigeno | 27 % Show Supplier Material materials with Índice límite de óxigeno of 27 % | dry | ISO 4589-1/-2 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 66 % Show Supplier Material materials with Elongación of 66 % | dry | ISO 527-1/-2 |
50 % Show Supplier Material materials with Elongación of 50 % | dry, conditioned | ISO 527-1/-2 | ||
120 °C | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
160 °C | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
Elongation at yield | 20 % Show Supplier Material materials with Elongation at yield of 20 % | dry | ISO 527-1/-2 | |
25 % Show Supplier Material materials with Elongation at yield of 25 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 40 MPa Show Supplier Material materials with Flexural yield strength of 40 MPa | conditioned | ISO 178 | |
80 MPa Show Supplier Material materials with Flexural yield strength of 80 MPa | dry | ISO 178 | ||
120 °C | 40 MPa Show Supplier Material materials with Flexural yield strength of 40 MPa | dry | ISO 178 | |
160 °C | 30 MPa Show Supplier Material materials with Flexural yield strength of 30 MPa | dry | ISO 178 | |
Límite elástico | 45 MPa Show Supplier Material materials with Límite elástico of 45 MPa | conditioned | ISO 527-1/-2 | |
60 MPa Show Supplier Material materials with Límite elástico of 60 MPa | dry | ISO 527-1/-2 | ||
120 °C | 35 MPa Show Supplier Material materials with Límite elástico of 35 MPa | dry | ISO 527-1/-2 | |
160 °C | 30 MPa Show Supplier Material materials with Límite elástico of 30 MPa | dry | ISO 527-1/-2 | |
Módulo de flexión | 0.55 GPa Show Supplier Material materials with Módulo de flexión of 0.55 GPa | conditioned | ISO 178 | |
1.8 GPa Show Supplier Material materials with Módulo de flexión of 1.8 GPa | dry | ISO 178 | ||
120 °C | 0.4 GPa Show Supplier Material materials with Módulo de flexión of 0.4 GPa | dry | ISO 178 | |
160 °C | 0.35 GPa Show Supplier Material materials with Módulo de flexión of 0.35 GPa | dry | ISO 178 | |
Módulo elástico | 0.6 GPa Show Supplier Material materials with Módulo elástico of 0.6 GPa | conditioned | ISO 527-1/-2 | |
1.9 GPa Show Supplier Material materials with Módulo elástico of 1.9 GPa | dry | ISO 527-1/-2 | ||
120 °C | 0.4 GPa Show Supplier Material materials with Módulo elástico of 0.4 GPa | dry | ISO 527-1/-2 | |
160 °C | 0.35 GPa Show Supplier Material materials with Módulo elástico of 0.35 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | -40 °C | 85 MPa Show Supplier Material materials with Resistencia a la tracción of 85 MPa | dry | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 26 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 26 kJ/m² | dry | ISO 179/1eA |
-30 °C | 30 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 30 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 75 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 75 kJ/m² | dry | ISO 179/1eA | |
23 °C | 125 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 125 kJ/m² | conditioned | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1.6e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.6e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
1.8e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.8e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Difusividad térmica | 9.82e-07 mm²/s Show Supplier Material materials with Difusividad térmica of 9.82e-07 mm²/s | dry | - | ||
Temperatura de flexión bajo carga | 90 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 90 °C | dry | ISO 75-1/-2 | 2 MPa | |
200 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 200 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de reblandecimiento Vicat | 250 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 250 °C | dry | ISO 306 | 50°C/h 50N | |
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.2 [-] Show Supplier Material materials with Constante dieléctrica of 3.2 [-] | dry | IEC 62631-2-1 | 1MHz |
3.6 [-] Show Supplier Material materials with Constante dieléctrica of 3.6 [-] | dry | IEC 62631-2-1 | 100Hz | |
4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
14.0 [-] Show Supplier Material materials with Constante dieléctrica of 14.0 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 120 [-] Show Supplier Material materials with Factor de disipación of 120 [-] | dry | IEC 62631-2-1 | 100Hz |
190 [-] Show Supplier Material materials with Factor de disipación of 190 [-] | dry | IEC 62631-2-1 | 1MHz | |
1000 [-] Show Supplier Material materials with Factor de disipación of 1000 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
6500 [-] Show Supplier Material materials with Factor de disipación of 6500 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Rigidez dieléctrica | 15 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 15 kV/mm | conditioned | IEC 60243-1 | |
25 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 25 kV/mm | dry | IEC 60243-1 | ||
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+07 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+07 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | ||
Índice de seguimiento comparativo | 475 V Show Supplier Material materials with Índice de seguimiento comparativo of 475 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 2 % Show Supplier Material materials with Contracción of 2 % | dry | Sim. to ISO 294-4 | Parallel |
2 % Show Supplier Material materials with Contracción of 2 % | dry | Sim. to ISO 294-4 | Normal | |
Density of melt | 913 g/cm³ Show Supplier Material materials with Density of melt of 913 g/cm³ | dry | - | |
Specific heat capacity melt | 2550 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2550 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.24 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.24 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Convoluted Tubes, Front End Accessory Drive Parts: Belt Tensioner,Damping bands, Shoes and Bushings |