General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.35 % Show Supplier Material materials with Absorción de agua of 0.35 % | dry | Sim. to ISO 62 |
Densidad | 1.48 g/cm³ Show Supplier Material materials with Densidad of 1.48 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2.2 % Show Supplier Material materials with Elongación of 2.2 % | dry | ISO 527-1/-2 | |
Módulo elástico | 4.5 GPa Show Supplier Material materials with Módulo elástico of 4.5 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 55.0 MPa Show Supplier Material materials with Resistencia a la tracción of 55.0 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 2 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 2 kJ/m² | dry | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 30 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 30 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 100 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 100 °C | dry | ISO 75-1/-2 | 2 MPa | |
195 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 195 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 225 °C Show Supplier Material materials with Temperatura de fusión of 225 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.4 % Show Supplier Material materials with Contracción of 1.4 % | dry | Sim. to ISO 294-4 | Parallel | |
1.7 % Show Supplier Material materials with Contracción of 1.7 % | dry | Sim. to ISO 294-4 | Normal | ||
Velocidad de flujo del volumen derretido | 270 °C | 34 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 34 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Fillers | 20% Mineral Powder |