General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.75 % Show Supplier Material materials with Absorción de agua of 0.75 % | dry | Sim. to ISO 62 |
Densidad | 0.69 g/cm³ Show Supplier Material materials with Densidad of 0.69 g/cm³ | dry | ISO 60 |
1.11 g/cm³ Show Supplier Material materials with Densidad of 1.11 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.3 % Show Supplier Material materials with Moisture absorption of 0.3 % | dry | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 33 [-] Show Supplier Material materials with Dureza Shore D of 33 [-] | dry | ISO 868 | 3s |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
300 % Show Supplier Material materials with Elongación of 300 % | dry | ISO 527-1/-2 | ||
Elongation at yield | 77 % Show Supplier Material materials with Elongation at yield of 77 % | dry | ISO 527-1/-2 | |
Módulo elástico | 0.04 GPa Show Supplier Material materials with Módulo elástico of 0.04 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 21 MPa Show Supplier Material materials with Resistencia a la tracción of 21 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2.2e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
2.2e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Difusividad térmica | 6.56e-08 mm²/s Show Supplier Material materials with Difusividad térmica of 6.56e-08 mm²/s | dry | - | ||
Inflamabilidad | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes |
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | UL746B | 2 mm | |
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | UL746B | 2 mm | |
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | UL746B | 2 mm | |
Temperatura de fusión | 195 °C Show Supplier Material materials with Temperatura de fusión of 195 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | -78 °C Show Supplier Material materials with Temperatura de transición del vidrio of -78 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.1 [-] Show Supplier Material materials with Constante dieléctrica of 4.1 [-] | dry | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 10 [-] Show Supplier Material materials with Factor de disipación of 10 [-] | dry | IEC 62631-2-1 | 100Hz |
170 [-] Show Supplier Material materials with Factor de disipación of 170 [-] | dry | IEC 62631-2-1 | 1MHz | |
Rigidez dieléctrica | 20 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20 kV/mm | dry | IEC 60243-1 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.5 % Show Supplier Material materials with Contracción of 1.5 % | dry | Sim. to ISO 294-4 | Parallel | |
1.5 % Show Supplier Material materials with Contracción of 1.5 % | dry | Sim. to ISO 294-4 | Normal | ||
Density of melt | 896 g/cm³ Show Supplier Material materials with Density of melt of 896 g/cm³ | dry | - | ||
Specific heat capacity melt | 1700.0 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1700.0 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.1 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.1 W/(m·K) | dry | - | ||
Velocidad de flujo del volumen derretido | 230 °C | 33 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 33 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Washing Machine Timer Knobs, Screw Drivers and Plyers, Chair Carriers, Seat Suspension/Fabrics, Soft touch in spatulas and kitchenware, Railway Pads, Conveyor Belts, Arnitel spring in monitor arm, Cosmetic Dispensers, Wine Taps, Grips, Industrial Cords and Ropes, Support Springs, Phone case | |
Certifications | Food Contact, USP class VI, Yellow Card Available |