General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.7 % Show Supplier Material materials with Absorción de agua of 0.7 % | dry | Sim. to ISO 62 |
Densidad | 1.15 g/cm³ Show Supplier Material materials with Densidad of 1.15 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.3 % Show Supplier Material materials with Moisture absorption of 0.3 % | dry | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 39 [-] Show Supplier Material materials with Dureza Shore D of 39 [-] | dry | ISO 868 | 3s |
39 [-] Show Supplier Material materials with Dureza Shore D of 39 [-] | dry | ISO 868 | 15s | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
300 % Show Supplier Material materials with Elongación of 300 % | dry | ISO 527-1/-2 | ||
950 % Show Supplier Material materials with Elongación of 950 % | dry | ISO 527-1/-2 | ||
Módulo elástico | 0.07 GPa Show Supplier Material materials with Módulo elástico of 0.07 GPa | dry | ISO 527-1/-2 | |
Resistencia a desgarros | 95 kN/m Show Supplier Material materials with Resistencia a desgarros of 95 kN/m | dry | ISO 34-1; Method B | |
260 kN/m Show Supplier Material materials with Resistencia a desgarros of 260 kN/m | dry | ISO 34-1; Method B | ||
Resistencia a la tracción | 21.5 MPa Show Supplier Material materials with Resistencia a la tracción of 21.5 MPa | dry | ISO 527-1/-2 | |
32 MPa Show Supplier Material materials with Resistencia a la tracción of 32 MPa | dry | ISO 527-1/-2 | Normal |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Difusividad térmica | 8.6e-08 mm²/s Show Supplier Material materials with Difusividad térmica of 8.6e-08 mm²/s | dry | - | |
Temperatura de fusión | 213 °C Show Supplier Material materials with Temperatura de fusión of 213 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.5 % Show Supplier Material materials with Contracción of 1.5 % | dry | Sim. to ISO 294-4 | Parallel | |
2 % Show Supplier Material materials with Contracción of 2 % | dry | Sim. to ISO 294-4 | Normal | ||
Density of melt | 1010.0 g/cm³ Show Supplier Material materials with Density of melt of 1010.0 g/cm³ | dry | - | ||
Specific heat capacity melt | 2220 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2220 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.193 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.193 W/(m·K) | dry | - | ||
Velocidad de flujo del volumen derretido | 230 °C | 8 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 8 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Boots and Bellows |