General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 4.5 % Show Supplier Material materials with Absorción de agua of 4.5 % | dry | Sim. to ISO 62 |
Densidad | 1.55 g/cm³ Show Supplier Material materials with Densidad of 1.55 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.3 % Show Supplier Material materials with Moisture absorption of 1.3 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|---|
Elongación | 2 % Show Supplier Material materials with Elongación of 2 % | dry | 1 mm | ISO 527-1/-2 | ||
2.3 % Show Supplier Material materials with Elongación of 2.3 % | dry | ISO 527-1/-2 | ||||
2.8 % Show Supplier Material materials with Elongación of 2.8 % | conditioned | ISO 527-1/-2 | ||||
3.6 % Show Supplier Material materials with Elongación of 3.6 % | conditioned | ISO 527-1/-2 | ||||
120 °C | 6.3 % Show Supplier Material materials with Elongación of 6.3 % | dry | ISO 527-1/-2 | |||
160 °C | 8.1 % Show Supplier Material materials with Elongación of 8.1 % | dry | ISO 527-1/-2 | |||
Flexural yield strength | 165 MPa Show Supplier Material materials with Flexural yield strength of 165 MPa | conditioned | ISO 178 | |||
240 MPa Show Supplier Material materials with Flexural yield strength of 240 MPa | dry | ISO 178 | ||||
120 °C | 110 MPa Show Supplier Material materials with Flexural yield strength of 110 MPa | dry | ISO 178 | |||
160 °C | 75 MPa Show Supplier Material materials with Flexural yield strength of 75 MPa | dry | ISO 178 | |||
Módulo de flexión | 8 GPa Show Supplier Material materials with Módulo de flexión of 8 GPa | conditioned | ISO 178 | |||
11.5 GPa Show Supplier Material materials with Módulo de flexión of 11.5 GPa | dry | ISO 178 | ||||
120 °C | 5.7 GPa Show Supplier Material materials with Módulo de flexión of 5.7 GPa | dry | ISO 178 | |||
160 °C | 4.1 GPa Show Supplier Material materials with Módulo de flexión of 4.1 GPa | dry | ISO 178 | |||
Módulo elástico | 8 GPa Show Supplier Material materials with Módulo elástico of 8 GPa | conditioned | ISO 527-1/-2 | |||
8.3 GPa Show Supplier Material materials with Módulo elástico of 8.3 GPa | conditioned | ISO 527-1/-2 | ||||
12 GPa Show Supplier Material materials with Módulo elástico of 12 GPa | dry | ISO 527-1/-2 | ||||
12 GPa Show Supplier Material materials with Módulo elástico of 12 GPa | dry | 1 mm | ISO 527-1/-2 | |||
120 °C | 5.4 GPa Show Supplier Material materials with Módulo elástico of 5.4 GPa | dry | ISO 527-1/-2 | |||
160 °C | 3.5 GPa Show Supplier Material materials with Módulo elástico of 3.5 GPa | dry | ISO 527-1/-2 | |||
Resistencia a la tracción | 95 MPa Show Supplier Material materials with Resistencia a la tracción of 95 MPa | conditioned | ISO 527-1/-2 | at low thickness | ||
105 MPa Show Supplier Material materials with Resistencia a la tracción of 105 MPa | conditioned | ISO 527-1/-2 | ||||
150 MPa Show Supplier Material materials with Resistencia a la tracción of 150 MPa | dry | 1 mm | ISO 527-1/-2 | at low thickness | ||
155 MPa Show Supplier Material materials with Resistencia a la tracción of 155 MPa | dry | ISO 527-1/-2 | ||||
120 °C | 75 MPa Show Supplier Material materials with Resistencia a la tracción of 75 MPa | dry | ISO 527-1/-2 | |||
160 °C | 55.0 MPa Show Supplier Material materials with Resistencia a la tracción of 55.0 MPa | dry | ISO 527-1/-2 | |||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | dry, conditioned | ISO 179/1eA | ||
23 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | dry | ISO 179/1eA | |||
23 °C | 14.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14.0 kJ/m² | conditioned | ISO 179/1eA | |||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m² | dry, conditioned | ISO 179/1eU | ||
23 °C | 55.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 55.0 kJ/m² | dry, conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Ball pressure temperature | 210 °C Show Supplier Material materials with Ball pressure temperature of 210 °C | dry | IEC 60695-10-2 | |||
Coeficiente de dilatación térmica | 2e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
1.1e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.1e-06 1/K | dry | ISO 11359-1/-2 | Normal | |||
Difusividad térmica | 1.2e-07 mm²/s Show Supplier Material materials with Difusividad térmica of 1.2e-07 mm²/s | dry | - | |||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.75 mm | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 3 mm | |||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | dry | IEC 60695-2-13 | 0.75 mm | ||
800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | dry | IEC 60695-2-13 | 2 mm | |||
Inflamabilidad | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
5VA | dry | IEC 60695-11-20 | 1.5 mm | |||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | dry | UL746B | 0.75 mm | ||
Temperatura de flexión bajo carga | 205 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 205 °C | dry | ISO 75-1/-2 | 2 MPa | ||
215 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 215 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.4 [-] Show Supplier Material materials with Constante dieléctrica of 3.4 [-] | dry | IEC 62631-2-1 | 1MHz |
3.5 [-] Show Supplier Material materials with Constante dieléctrica of 3.5 [-] | dry | IEC 62631-2-1 | 100Hz | |
4 [-] Show Supplier Material materials with Constante dieléctrica of 4 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
10 [-] Show Supplier Material materials with Constante dieléctrica of 10 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 60 [-] Show Supplier Material materials with Factor de disipación of 60 [-] | dry | IEC 62631-2-1 | 100Hz |
120 [-] Show Supplier Material materials with Factor de disipación of 120 [-] | dry | IEC 62631-2-1 | 1MHz | |
700 [-] Show Supplier Material materials with Factor de disipación of 700 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3000 [-] Show Supplier Material materials with Factor de disipación of 3000 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | ||
Índice de seguimiento comparativo | 325 V Show Supplier Material materials with Índice de seguimiento comparativo of 325 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.21 % Show Supplier Material materials with Contracción of 0.21 % | dry | Sim. to ISO 294-4 | Parallel |
0.77 % Show Supplier Material materials with Contracción of 0.77 % | dry | Sim. to ISO 294-4 | Normal | |
Density of melt | 1150 g/cm³ Show Supplier Material materials with Density of melt of 1150 g/cm³ | dry | - | |
Specific heat capacity melt | 1900 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1900 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.26 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.26 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Photovoltaic connector, EV Charging Plugs | |
Certifications | VDE, Yellow Card Available | |
Fillers | 30% Glass Fiber |