General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 45 [-] Show Supplier Material materials with Dureza Shore D of 45 [-] | dry | ISO 868 | 3s |
Elongación | 350 % Show Supplier Material materials with Elongación of 350 % | dry | ISO 527-1/-2 | |
Módulo elástico | 0.14 GPa Show Supplier Material materials with Módulo elástico of 0.14 GPa | dry | ISO 527-1/-2 | |
Resistencia a desgarros | 94 kN/m Show Supplier Material materials with Resistencia a desgarros of 94 kN/m | dry | ISO 34-1; Method B | |
Resistencia a la tracción | 21 MPa Show Supplier Material materials with Resistencia a la tracción of 21 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 65 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 65 °C | dry | ISO 75-1/-2 | 0.45 MPa | |
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de reblandecimiento Vicat | 189 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 189 °C | dry | ISO 306 | 50°C/h 10N |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.6 % Show Supplier Material materials with Contracción of 1.6 % | dry | Sim. to ISO 294-4 | Parallel | |
1.8 % Show Supplier Material materials with Contracción of 1.8 % | dry | Sim. to ISO 294-4 | Normal | ||
Velocidad de flujo del volumen derretido | 230 °C | 39 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 39 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Bed Springs, Railway Pads, Cosmetic Dispensers, Soap dispensers, Support Springs, Non-pneumatic wheel, Non-pneumatic wheel |