General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 5.8 % Show Supplier Material materials with Absorción de agua of 5.8 % | dry | Sim. to ISO 62 |
Densidad | 1.39 g/cm³ Show Supplier Material materials with Densidad of 1.39 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.65 % Show Supplier Material materials with Moisture absorption of 1.65 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 3 % Show Supplier Material materials with Elongación of 3 % | dry | ISO 527-1/-2 | |
5 % Show Supplier Material materials with Elongación of 5 % | conditioned | ISO 527-1/-2 | ||
Módulo de flexión | 9.1 GPa Show Supplier Material materials with Módulo de flexión of 9.1 GPa | dry | ISO 178 | |
Módulo elástico | 6.5 GPa Show Supplier Material materials with Módulo elástico of 6.5 GPa | conditioned | ISO 527-1/-2 | |
10.5 GPa Show Supplier Material materials with Módulo elástico of 10.5 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 120 MPa Show Supplier Material materials with Resistencia a la tracción of 120 MPa | conditioned | ISO 527-1/-2 | |
170 MPa Show Supplier Material materials with Resistencia a la tracción of 170 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 9.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9.5 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 210 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 210 °C | dry | ISO 75-1/-2 | 2 MPa | |
220 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Fillers | 33% Glass Fiber |