General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 5.8 % Show Supplier Material materials with Absorción de agua of 5.8 % | dry | Sim. to ISO 62 |
Bio-based content | 70 % Show Supplier Material materials with Bio-based content of 70 % | dry | ASTM D6866-12 Method B |
Densidad | 1.09 g/cm³ Show Supplier Material materials with Densidad of 1.09 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.9 % Show Supplier Material materials with Moisture absorption of 1.9 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 20 % Show Supplier Material materials with Elongación of 20 % | dry | ISO 527-1/-2 | |
50 % Show Supplier Material materials with Elongación of 50 % | conditioned | ISO 527-1/-2 | ||
120 °C | 200 % Show Supplier Material materials with Elongación of 200 % | dry | ISO 527-1/-2 | |
140 °C | 200 % Show Supplier Material materials with Elongación of 200 % | dry | ISO 527-1/-2 | |
Elongation at yield | 4.6 % Show Supplier Material materials with Elongation at yield of 4.6 % | dry | ISO 527-1/-2 | |
20 % Show Supplier Material materials with Elongation at yield of 20 % | conditioned | ISO 527-1/-2 | ||
Módulo elástico | 1.6 GPa Show Supplier Material materials with Módulo elástico of 1.6 GPa | conditioned | ISO 527-1/-2 | |
3.2 GPa Show Supplier Material materials with Módulo elástico of 3.2 GPa | dry | ISO 527-1/-2 | ||
120 °C | 0.6 GPa Show Supplier Material materials with Módulo elástico of 0.6 GPa | dry | ISO 527-1/-2 | |
140 °C | 0.52 GPa Show Supplier Material materials with Módulo elástico of 0.52 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 45 MPa Show Supplier Material materials with Resistencia a la tracción of 45 MPa | conditioned | ISO 527-1/-2 | |
55.0 MPa Show Supplier Material materials with Resistencia a la tracción of 55.0 MPa | dry | ISO 527-1/-2 | ||
120 °C | 38 MPa Show Supplier Material materials with Resistencia a la tracción of 38 MPa | dry | ISO 527-1/-2 | |
140 °C | 32 MPa Show Supplier Material materials with Resistencia a la tracción of 32 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | dry | ISO 179/1eA |
-30 °C | 4.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4.5 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 5.5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | conditioned | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 75 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 75 °C | dry | ISO 75-1/-2 | 2 MPa | |
175 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 175 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 250 °C Show Supplier Material materials with Temperatura de fusión of 250 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo de la masa derretida | 280 °C | 24 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 24 g/10min | dry | ISO 1133 |
Velocidad de flujo del volumen derretido | 280 °C | 26 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 26 cm³/10min | dry | ISO 1133 |
Viscosity number | 170 cm³/gr Show Supplier Material materials with Viscosity number of 170 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property |
---|