General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 0.4 % Show Supplier Material materials with Absorción de agua of 0.4 % | dry | Sim. to ISO 62 |
Densidad | 1.73 g/cm³ Show Supplier Material materials with Densidad of 1.73 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.12 % Show Supplier Material materials with Moisture absorption of 0.12 % | dry | Sim. to ISO 62 |
Índice límite de óxigeno | 36 % Show Supplier Material materials with Índice límite de óxigeno of 36 % | dry | ISO 4589-1/-2 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2 % Show Supplier Material materials with Elongación of 2 % | dry | ISO 527-1/-2 | |
Módulo elástico | 13 GPa Show Supplier Material materials with Módulo elástico of 13 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 160 MPa Show Supplier Material materials with Resistencia a la tracción of 160 MPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | dry | ISO 179/1eA |
23 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 35 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 35 kJ/m² | dry | ISO 179/1eU |
23 °C | 35 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 35 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
6.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Difusividad térmica | 8.67e-08 mm²/s Show Supplier Material materials with Difusividad térmica of 8.67e-08 mm²/s | dry | - | |||
Inflamabilidad | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 150 °C Show Supplier Material materials with Relative temperature index, electrical of 150 °C | dry | UL746B | 0.71 mm | ||
Relative temperature index, mechanical impact | 125 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 125 °C | dry | UL746B | 0.71 mm | ||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | UL746B | 0.71 mm | ||
Temperatura de flexión bajo carga | 220 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 220 °C | dry | ISO 75-1/-2 | 2 MPa | ||
240 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 240 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 255 °C Show Supplier Material materials with Temperatura de fusión of 255 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.4 [-] Show Supplier Material materials with Constante dieléctrica of 3.4 [-] | dry | IEC 62631-2-1 | 1MHz |
3.7 [-] Show Supplier Material materials with Constante dieléctrica of 3.7 [-] | dry | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 10 [-] Show Supplier Material materials with Factor de disipación of 10 [-] | dry | IEC 62631-2-1 | 100Hz |
120 [-] Show Supplier Material materials with Factor de disipación of 120 [-] | dry | IEC 62631-2-1 | 1MHz | |
Rigidez dieléctrica | 29.0 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 29.0 kV/mm | dry | IEC 60243-1 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | |
Índice de seguimiento comparativo | 225 V Show Supplier Material materials with Índice de seguimiento comparativo of 225 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | dry | ISO 294-4 | Parallel |
1 % Show Supplier Material materials with Contracción of 1 % | dry | ISO 294-4 | Normal | |
Density of melt | 1350 g/cm³ Show Supplier Material materials with Density of melt of 1350 g/cm³ | dry | - | |
Specific heat capacity melt | 1670 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1670 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.195 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.195 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 33% Glass Fiber |