General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 3.9 % Show Supplier Material materials with Absorción de agua of 3.9 % | dry | Sim. to ISO 62 |
Densidad | 1.62 g/cm³ Show Supplier Material materials with Densidad of 1.62 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2.6 % Show Supplier Material materials with Elongación of 2.6 % | dry, conditioned | ISO 527-1/-2 | |
Módulo elástico | 17.5 GPa Show Supplier Material materials with Módulo elástico of 17.5 GPa | dry, conditioned | ISO 527-1/-2 | |
Resistencia a la tracción | 280 MPa Show Supplier Material materials with Resistencia a la tracción of 280 MPa | dry, conditioned | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | 23 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 295 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 295 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 315 °C Show Supplier Material materials with Temperatura de fusión of 315 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 130 °C Show Supplier Material materials with Temperatura de transición del vidrio of 130 °C | dry | ASTM D5026/D7028 | DMTA (tan d) |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 50% Glass Fiber |