General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 3.6 % Show Supplier Material materials with Absorción de agua of 3.6 % | dry | Sim. to ISO 62 |
Densidad | 1.7 g/cm³ Show Supplier Material materials with Densidad of 1.7 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1 % Show Supplier Material materials with Moisture absorption of 1 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2.2 % Show Supplier Material materials with Elongación of 2.2 % | dry | ISO 527-1/-2 | |
4 % Show Supplier Material materials with Elongación of 4 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 365 MPa Show Supplier Material materials with Flexural yield strength of 365 MPa | dry | ISO 178 | |
Módulo de flexión | 18.5 GPa Show Supplier Material materials with Módulo de flexión of 18.5 GPa | dry | ISO 178 | |
Módulo elástico | 14 GPa Show Supplier Material materials with Módulo elástico of 14 GPa | conditioned | ISO 527-1/-2 | |
20 GPa Show Supplier Material materials with Módulo elástico of 20 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 160 MPa Show Supplier Material materials with Resistencia a la tracción of 160 MPa | conditioned | ISO 527-1/-2 | |
240 MPa Show Supplier Material materials with Resistencia a la tracción of 240 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | dry | ISO 179/1eA | |
23 °C | 25 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 25 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 85 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 85 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 90 kJ/m² | dry | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 100 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
4e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Difusividad térmica | 1.64e-07 mm²/s Show Supplier Material materials with Difusividad térmica of 1.64e-07 mm²/s | dry | - | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.75 mm | ||
Temperatura de flexión bajo carga | 210 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 210 °C | dry | ISO 75-1/-2 | 2 MPa | ||
220 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | dry | ISO 294-4 | Parallel |
0.8 % Show Supplier Material materials with Contracción of 0.8 % | dry | ISO 294-4 | Normal | |
Density of melt | 1380.0 g/cm³ Show Supplier Material materials with Density of melt of 1380.0 g/cm³ | dry | - | |
Specific heat capacity melt | 1720.0 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1720.0 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.39 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.39 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 60% Glass Fiber |