General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Absorción de agua | 7 % Show Supplier Material materials with Absorción de agua of 7 % | dry | Sim. to ISO 62 |
Densidad | 1.06 g/cm³ Show Supplier Material materials with Densidad of 1.06 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.5 % Show Supplier Material materials with Moisture absorption of 2.5 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 30 % Show Supplier Material materials with Elongación of 30 % | dry | ISO 527-1/-2 |
50 % Show Supplier Material materials with Elongación of 50 % | dry, conditioned | ISO 527-1/-2 | ||
Elongation at yield | -40 °C | 9 % Show Supplier Material materials with Elongation at yield of 9 % | dry | ISO 527-1/-2 |
4.2 % Show Supplier Material materials with Elongation at yield of 4.2 % | dry | ISO 527-1/-2 | ||
Flexural yield strength | 20 MPa Show Supplier Material materials with Flexural yield strength of 20 MPa | conditioned | ISO 178 | |
63 MPa Show Supplier Material materials with Flexural yield strength of 63 MPa | dry | ISO 178 | ||
Límite elástico | -40 °C | 71 MPa Show Supplier Material materials with Límite elástico of 71 MPa | dry | ISO 527-1/-2 |
43 MPa Show Supplier Material materials with Límite elástico of 43 MPa | dry | ISO 527-1/-2 | ||
Módulo de flexión | 0.5 GPa Show Supplier Material materials with Módulo de flexión of 0.5 GPa | conditioned | ISO 178 | |
1.7 GPa Show Supplier Material materials with Módulo de flexión of 1.7 GPa | dry | ISO 178 | ||
Módulo elástico | -40 °C | 2 GPa Show Supplier Material materials with Módulo elástico of 2 GPa | dry | ISO 527-1/-2 |
0.53 GPa Show Supplier Material materials with Módulo elástico of 0.53 GPa | conditioned | ISO 527-1/-2 | ||
1.8 GPa Show Supplier Material materials with Módulo elástico of 1.8 GPa | dry | ISO 527-1/-2 | ||
Puncture energy | -40 °C | 65 J Show Supplier Material materials with Puncture energy of 65 J | dry | ISO 6603-2 |
23 °C | 48 J Show Supplier Material materials with Puncture energy of 48 J | dry | ISO 6603-2 | |
Puncture force | -40 °C | 5000 N Show Supplier Material materials with Puncture force of 5000 N | dry | ISO 6603-2 |
23 °C | 3300 N Show Supplier Material materials with Puncture force of 3300 N | dry | ISO 6603-2 | |
Resistencia a la tracción | -40 °C | 55.0 MPa Show Supplier Material materials with Resistencia a la tracción of 55.0 MPa | dry | ISO 527-1/-2 |
37 MPa Show Supplier Material materials with Resistencia a la tracción of 37 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 20 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 20 kJ/m² | conditioned | ISO 179/1eA |
-30 °C | 22 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 22 kJ/m² | dry | ISO 179/1eA | |
23 °C | 80 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 80 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
1.1e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.1e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Difusividad térmica | 9.37e-08 mm²/s Show Supplier Material materials with Difusividad térmica of 9.37e-08 mm²/s | dry | - | ||
Temperatura de flexión bajo carga | 55 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 55 °C | dry | ISO 75-1/-2 | 2 MPa | |
100 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 100 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de reblandecimiento Vicat | 130 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 130 °C | dry | ISO 306 | 50°C/h 50N |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 1.8 % Show Supplier Material materials with Contracción of 1.8 % | dry | ISO 294-4 | Normal | |
1.9 % Show Supplier Material materials with Contracción of 1.9 % | dry | ISO 294-4 | Parallel | ||
Density of melt | 869 g/cm³ Show Supplier Material materials with Density of melt of 869 g/cm³ | dry | - | ||
Specific heat capacity melt | 2740 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2740 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.22 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.22 W/(m·K) | dry | - | ||
Velocidad de flujo del volumen derretido | 250 °C | 13 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 13 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Outdoor power product fuel tanks, High pressure type IV composite fuel tanks |