General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 0.4 % Show Supplier Material materials with Absorción de agua of 0.4 % | dry | ISO 62 | at 23°C after 24h |
5.1 % Show Supplier Material materials with Absorción de agua of 5.1 % | dry | Sim. to ISO 62 | ||
Densidad | 1.43 g/cm³ Show Supplier Material materials with Densidad of 1.43 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Elongación | -40 °C | 2.3 % Show Supplier Material materials with Elongación of 2.3 % | dry | ISO 527-1/-2 | ||
2 % Show Supplier Material materials with Elongación of 2 % | conditioned | ISO 527-1/-2 | ||||
2.2 % Show Supplier Material materials with Elongación of 2.2 % | dry | ISO 527-1/-2 | ||||
2.5 % Show Supplier Material materials with Elongación of 2.5 % | dry, conditioned | ISO 527-1/-2 | 1 mm | |||
40 °C | 2.3 % Show Supplier Material materials with Elongación of 2.3 % | dry | ISO 527-1/-2 | |||
80 °C | 2.6 % Show Supplier Material materials with Elongación of 2.6 % | dry | ISO 527-1/-2 | |||
80 °C | 6 % Show Supplier Material materials with Elongación of 6 % | conditioned | ISO 527-1/-2 | |||
100 °C | 3.2 % Show Supplier Material materials with Elongación of 3.2 % | dry | ISO 527-1/-2 | |||
120 °C | 4.3 % Show Supplier Material materials with Elongación of 4.3 % | dry | ISO 527-1/-2 | |||
120 °C | 5 % Show Supplier Material materials with Elongación of 5 % | conditioned | ISO 527-1/-2 | |||
150 °C | 6 % Show Supplier Material materials with Elongación of 6 % | dry | ISO 527-1/-2 | |||
160 °C | 6 % Show Supplier Material materials with Elongación of 6 % | dry | ISO 527-1/-2 | |||
180 °C | 6 % Show Supplier Material materials with Elongación of 6 % | dry | ISO 527-1/-2 | |||
200 °C | 6 % Show Supplier Material materials with Elongación of 6 % | dry | ISO 527-1/-2 | |||
210 °C | 0.006 % Show Supplier Material materials with Elongación of 0.006 % | dry | ISO 527-1/-2 | |||
Flexural yield strength | 260 MPa Show Supplier Material materials with Flexural yield strength of 260 MPa | conditioned | ISO 178 | |||
300 MPa Show Supplier Material materials with Flexural yield strength of 300 MPa | dry | ISO 178 | ||||
80 °C | 150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | conditioned | ISO 178 | |||
80 °C | 260 MPa Show Supplier Material materials with Flexural yield strength of 260 MPa | dry | ISO 178 | |||
120 °C | 180 MPa Show Supplier Material materials with Flexural yield strength of 180 MPa | dry | ISO 178 | |||
160 °C | 120 MPa Show Supplier Material materials with Flexural yield strength of 120 MPa | dry | ISO 178 | |||
180 °C | 110 MPa Show Supplier Material materials with Flexural yield strength of 110 MPa | dry | ISO 178 | |||
200 °C | 100 MPa Show Supplier Material materials with Flexural yield strength of 100 MPa | dry | ISO 178 | |||
210 °C | 95 MPa Show Supplier Material materials with Flexural yield strength of 95 MPa | dry | ISO 178 | |||
Módulo de flexión | 10.5 GPa Show Supplier Material materials with Módulo de flexión of 10.5 GPa | dry | ISO 178 | |||
11 GPa Show Supplier Material materials with Módulo de flexión of 11 GPa | conditioned | ISO 178 | ||||
80 °C | 6 GPa Show Supplier Material materials with Módulo de flexión of 6 GPa | conditioned | ISO 178 | |||
80 °C | 10 GPa Show Supplier Material materials with Módulo de flexión of 10 GPa | dry | ISO 178 | |||
120 °C | 7.6 GPa Show Supplier Material materials with Módulo de flexión of 7.6 GPa | dry | ISO 178 | |||
160 °C | 4.5 GPa Show Supplier Material materials with Módulo de flexión of 4.5 GPa | dry | ISO 178 | |||
180 °C | 4.2 GPa Show Supplier Material materials with Módulo de flexión of 4.2 GPa | dry | ISO 178 | |||
200 °C | 4 GPa Show Supplier Material materials with Módulo de flexión of 4 GPa | dry | ISO 178 | |||
210 °C | 3.8 GPa Show Supplier Material materials with Módulo de flexión of 3.8 GPa | dry | ISO 178 | |||
Módulo elástico | -40 °C | 11.5 GPa Show Supplier Material materials with Módulo elástico of 11.5 GPa | dry | ISO 527-1/-2 | ||
10.8 GPa Show Supplier Material materials with Módulo elástico of 10.8 GPa | dry | ISO 527-1/-2 | 1 mm | |||
11 GPa Show Supplier Material materials with Módulo elástico of 11 GPa | conditioned | ISO 527-1/-2 | ||||
11.3 GPa Show Supplier Material materials with Módulo elástico of 11.3 GPa | dry | ISO 527-1/-2 | ||||
11.5 GPa Show Supplier Material materials with Módulo elástico of 11.5 GPa | conditioned | ISO 527-1/-2 | ||||
40 °C | 10.8 GPa Show Supplier Material materials with Módulo elástico of 10.8 GPa | dry | ISO 527-1/-2 | |||
80 °C | 6.2 GPa Show Supplier Material materials with Módulo elástico of 6.2 GPa | conditioned | ISO 527-1/-2 | |||
80 °C | 10.5 GPa Show Supplier Material materials with Módulo elástico of 10.5 GPa | dry | ISO 527-1/-2 | |||
100 °C | 10 GPa Show Supplier Material materials with Módulo elástico of 10 GPa | dry | ISO 527-1/-2 | |||
120 °C | 4.6 GPa Show Supplier Material materials with Módulo elástico of 4.6 GPa | conditioned | ISO 527-1/-2 | |||
120 °C | 8 GPa Show Supplier Material materials with Módulo elástico of 8 GPa | dry | ISO 527-1/-2 | |||
150 °C | 5 GPa Show Supplier Material materials with Módulo elástico of 5 GPa | dry | ISO 527-1/-2 | |||
160 °C | 4.5 GPa Show Supplier Material materials with Módulo elástico of 4.5 GPa | dry | ISO 527-1/-2 | |||
180 °C | 4.3 GPa Show Supplier Material materials with Módulo elástico of 4.3 GPa | dry | ISO 527-1/-2 | |||
200 °C | 4 GPa Show Supplier Material materials with Módulo elástico of 4 GPa | dry | ISO 527-1/-2 | |||
210 °C | 3.9 GPa Show Supplier Material materials with Módulo elástico of 3.9 GPa | dry | ISO 527-1/-2 | |||
Resistencia a la tracción | -40 °C | 230 MPa Show Supplier Material materials with Resistencia a la tracción of 230 MPa | dry | ISO 527-1/-2 | ||
180 MPa Show Supplier Material materials with Resistencia a la tracción of 180 MPa | conditioned | ISO 527-1/-2 | ||||
190 MPa Show Supplier Material materials with Resistencia a la tracción of 190 MPa | conditioned | ISO 527-1/-2 | at low thickness | |||
200 MPa Show Supplier Material materials with Resistencia a la tracción of 200 MPa | dry | ISO 527-1/-2 | ||||
200 MPa Show Supplier Material materials with Resistencia a la tracción of 200 MPa | dry | ISO 527-1/-2 | 1 mm | at low thickness | ||
40 °C | 200 MPa Show Supplier Material materials with Resistencia a la tracción of 200 MPa | dry | ISO 527-1/-2 | |||
80 °C | 95 MPa Show Supplier Material materials with Resistencia a la tracción of 95 MPa | conditioned | ISO 527-1/-2 | |||
80 °C | 180 MPa Show Supplier Material materials with Resistencia a la tracción of 180 MPa | dry | ISO 527-1/-2 | |||
100 °C | 160 MPa Show Supplier Material materials with Resistencia a la tracción of 160 MPa | dry | ISO 527-1/-2 | |||
120 °C | 70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | conditioned | ISO 527-1/-2 | |||
120 °C | 130 MPa Show Supplier Material materials with Resistencia a la tracción of 130 MPa | dry | ISO 527-1/-2 | |||
150 °C | 95 MPa Show Supplier Material materials with Resistencia a la tracción of 95 MPa | dry | ISO 527-1/-2 | |||
160 °C | 90 MPa Show Supplier Material materials with Resistencia a la tracción of 90 MPa | dry | ISO 527-1/-2 | |||
180 °C | 80 MPa Show Supplier Material materials with Resistencia a la tracción of 80 MPa | dry | ISO 527-1/-2 | |||
200 °C | 70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | dry | ISO 527-1/-2 | |||
210 °C | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | dry | ISO 527-1/-2 | |||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | conditioned | ISO 179/1eA | ||
-30 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA | |||
23 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | conditioned | ISO 179/1eA | |||
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA | |||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 45 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 45 kJ/m² | conditioned | ISO 179/1eU | ||
-30 °C | 55.0 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 55.0 kJ/m² | dry | ISO 179/1eU | |||
23 °C | 50 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 50 kJ/m² | conditioned | ISO 179/1eU | |||
23 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 3.3e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.3e-07 1/K | dry | ASTM D696 | Parallel | |
4e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4e-07 1/K | dry | ASTM D696 | Normal | ||
Temperatura de flexión bajo carga | 305 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 305 °C | dry | ISO 75-1/-2 | 2 MPa | |
320 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 320 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 325 °C Show Supplier Material materials with Temperatura de fusión of 325 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperatura de transición del vidrio | 125 °C Show Supplier Material materials with Temperatura de transición del vidrio of 125 °C | dry | ISO 11357-1/-2 | 10°C/min | |
130 °C Show Supplier Material materials with Temperatura de transición del vidrio of 130 °C | dry | ASTM D5026/D7028 | DMTA (tan d) |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 35 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 35 kV/mm | dry, conditioned | IEC 60243-1 |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | conditioned | IEC 62631-3-2 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry, conditioned | IEC 62631-3-1 |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Faucet mixing valve, Panhandle, Bakeware | |
Certifications | Food Contact, Drinking Water, Yellow Card Available | |
Fillers | 30% Glass Fiber |