General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.21 g/cm³ Show Supplier Material materials with Densidad of 1.21 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 45 [-] Show Supplier Material materials with Dureza Shore D of 45 [-] | dry | ISO 868 | 3s |
Elongación | 205 % Show Supplier Material materials with Elongación of 205 % | dry | ISO 527-1/-2 | |
Módulo elástico | 0.12 GPa Show Supplier Material materials with Módulo elástico of 0.12 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 19.5 MPa Show Supplier Material materials with Resistencia a la tracción of 19.5 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 65 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 65 °C | dry | ISO 75-1/-2 | 0.45 MPa | |
Temperatura de fusión | 216 °C Show Supplier Material materials with Temperatura de fusión of 216 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 230 °C | 9.6 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 9.6 cm³/10min | dry | ISO 1133 |
Technological properties
Property |
---|